Teldene® H11BF
- Chemical Family
- PolyolefinsPolypropylenes (PP)
Teldene® H11BF is used as extrusion blown film for Food packaging, textile packaging film, packaging for hosiery, shirts, shopping bags and straws.
Properties
- Physical Form
- Granules
- Solid
Product families
Applications
- Food & Beverage Packaging
- Other Packaging Materials
Product Families
- Polyolefins
Other characteristics
- Brand
- Teldene
- Polymer Name
- Polypropylene Homopolymer (HPP)
- Melt Flow Index
- 11.0 - 11.0 g/10 min
- Additives Included
- Anti-Blocking Agent
- Processing Methods
- Extrusion, Film Extrusion
- Markets
- Printing & Packaging
- Technology
- Plastics
- Labeling Claims
- Food Contact Acceptable
- Food Regulations
This product is defined as a preparation under specific food contact regulation. Detailed information will be provided in a relevant document "Regulatory Compliances Product Declaration" upon request.
- Special Features
Shows broad processing window while providing good mechanical properties.
- Material Features
- Broad Processing Window
- Excellent Stiffness
- Food Contact Acceptable
- Good Mechanical Properties
- Good Processability
- High Clarity
- Key Characteristics
Excellent anti-blocking properties; High clarity; Good processability; Good stiffness; High slip; Food contact approval for specific applications (refer to NATPET)
- Storage and Handling
Polypropylene resin should be stored to prevent a direct exposure to sunlight and heat. The Product es-timated shelf life is one year starting from production date, adequate humidity below 80%, and tempera-ture below 40 oc. Customers might not fully follow the optimal storage condition, hence the shelf life recommended at customer site is six months only as received
- Processing Conditions
Averaqe extruder temperature ranqe may be kept between 220- 2300 °C . Quench temperature 33 °C
- Plastics and Elastomers End Uses
- Flexible Packaging
- Food Packaging
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
- Film Extrusion
Technical data
Table 1 of 1
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density 23°C | 0.9 | g/cm³ | ISO 1183 |
| Melt Flow Rate (MFR) 230°C/2.16 kg | 11 | g/10-min | ASTM D 1238-13 |
| Flexural Modulus | 1450 | MPa | ISO.178 |
| Tensile Stress at Yield 50-mm/min | 35 | MPa | ISO 527 |
| Tensile Strain at Yield 50-mm/min | 10 | % | ISO 527 |
| Iz0d Notched 23°C | 2.5 | KJ/㎡ | ISO 180 |
| Heat Deflection Temperature 0.45 MPa Un-annealed | 94 | °C | ISO 75B |
| Vicat Softening Temperature A50 (50°C/h 10N) | 155 | °C | ISO 306 |