Teldene® R25MLT
- Chemical Family
- PolyolefinsPolypropylenes (PP)
Teldene® R25MLT is suitable for thin walled is used as injection molding (TWIM) applications such as house wares, thin walled articles for food and non-food applications, video cassette cases, caps and lids, sports, leisure & toys and component parts for automotive industry.
Properties
- Physical Form
- Granules
- Solid
Product families
- Polyolefins
Other characteristics
- Brand
- Teldene
- Polymer Name
- Polypropylene Random Copolymer (RCP)
- Melt Flow Index
- 25.0 - 25.0 g/10 min
- Additives Included
- Anti-Static Agent, Nucleating Agent
- Anti-Static Agent
- Nucleating Agent
- Processing Methods
- Injection Molding
- Markets
- Automotive & Transportation
- Consumer Goods
- Printing & Packaging
- Technology
- Plastics
- Labeling Claims
- Food Contact Acceptable
- Food Regulations
This product is defined as a preparation under specific food contact regulation. Detailed information will be provided in a relevant document "Regulatory Compliances Product Declaration" upon request.
- Special Features
Amazing result on transparent articles; Shows broad processing window while providing excellent clarity at low molding temperature; Tested for biocompatibility, ISO 10993-4,5,10,11 (refer RCPD); Tested for VDA 270 compliance (refer RCPD)
- Material Features
- Biocompatible
- Broad Processing Window
- Dimensional Stability
- Excellent Transparency Properties
- Food Contact Acceptable
- Good Organoleptic Properties
- Low Energy Consumption
- Shorter Cycle Time
- Key Characteristics
Organoleptically suitable for food contact; Excellent transparency and dimensional stability; Nucleated & Anti-static additivated random copolymer; Potential for energy and cycle time saving; Suitable for defined medical/pharma-packing applications, subject to NATPET approval; Food contact approval for specific applications (refer to NATPET)
- Storage and Handling
Polypropylene resin should be stored to prevent a direct exposure to sunlight and heat. The Product estimated shelf life is one year starting from production date, adequate humidity below 80%, and temperature below 40°C. Customers might not fully follow the optimal storage condition, hence the shelf life recommended at customer site is six months only as received.
- Processing Conditions
Average extruder temperature range may be kept between 190 - 270°C.
- Plastics and Elastomers End Uses
- Caps
- Closures
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 1
15 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density 23°C | 0.9 | g/cm³ | ISO 1183 |
| Melt Flow Rate (MFR) 230°C/2.16 kg | 25 | g/10-min | ASTM D 1238-13 |
| Flexural Modulus | 1200 | MPa | ISO. 178 |
| Tensile Stress at Yield 50-mm/min | 29 | MPa | ISO 527 |
| Tensile Strain at Break 50-mm/min | min. 50 | % | ISO 527 |
| Tensile Strain at Yield 50-mm/min | 17 | % | ISO 527 |
| Charpy Un-notched 23 °C, Type 1, Edgewise | 200 | KJ/㎡ | ISO.179 |
| Charpy Un-notched O °C, Type 1, Edgewise | 70 | KJ/㎡ | ISO 179 |
| Charpy notched ,23 °C, Type 1, Edgewise | 6 | KJ/㎡ | ISO 179 |
| Charpy notched ,O °C, Type 1, Edgewise | 3 | KJ/㎡ | ISO 179 |
| Heat Deflection Temperature 0.45 MPa Un-annealed | 76 | °C | ISO 75B |
| Vicat Softening Temperature A50 (50°C/h 10N) | 130 | °c | ISO 306 |