To catalogue
Tasnee PP H2250
- Chemical Family
- PolyolefinsPolypropylenes (PP)
Tasnee PP H2250 is a Polypropylene Homopolymer with a Melt Flow Rate (MFR) of 25 g/10min. Tasnee PP H2250 is a medium narrow molecular weight distribution with anti-gas fading stabilization. It is intended for the extrusion of fine fibers with the spunbond technology for non-woven applications. It is also suitable for the extrusion of bulk continuous filament (BCF) for carpet pile and continuous filament (CF) yarns.
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Applications
- Consumer Goods — Apparel
- Consumer Goods — Carpet & Upholstery
Building & Construction — Decorative Materials & Finishes
- Carpet
Healthcare & Pharma — Medical
- Disposable Nonwovens
Personal Care — Personal Hygiene
- Baby Diapers
Product Families
Plastics — Basic Thermoplastics
- Polyolefins
Other characteristics
- Brand
- Tasnee PP
- Polymer Name
- Polypropylene Homopolymer (HPP)
- Melt Flow Index
- 25.0 - 25.0 g/10 min
- Processing Methods
- Extrusion, Injection Molding
- Color
- Translucent
- White
- Markets
- Building & Construction
- Consumer Goods
- Healthcare & Pharma
- Personal Care
- Technology
- Plastics
- Packaging Type
- Bags
- Material Features
- Good Color Stability
- Medium Molecular Weight
- Narrow Molecular Weight Distribution
- Odorless
- BCF Processing Conditions
Note: Processing parameters should only be used as guidelines. The above properties values are not to be construed as specifications.
- Plastics and Elastomers End Uses
- BCF Multifilament
- BCF Yarn
- Carpet Fiber
- Fibers
- Spunbond Nonwovens
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
- Injection Molding
Technical data
Table 1 of 2
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Charpy Notched Impact Strength (at 23°C) | 3 | kJ/m2 | ISO 179/1eA |
| Flexural Modulus (1% Secant) | 1450 | MPa | ISO 178 |
| Rockwell Hardness | 95 | R | ISO 2039-2 |
| Tensile Elongation at Yield | 10 | % | ISO 527-2 |
| Tensile Strength at Yield | 33 | MPa | ISO 527-2 |
Table 2 of 2
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 0.9 | g/cm3 | ISO 1183 |
| Heat Distortion Temperature (at 0.45 MPa) | 102 | °C | ISO 75-2 |
| Melt Flow Rate (230°C / 2.16 kg) | 25 | g / 10 min | ISO 1133 |
| Melting Temperature | 163 | °C | ISO 11357-3 |
| Vicat Softening Temperature | 152 | °C | ISO 306 |