To catalogue
Tasnee HDPE 100 Black
- Chemical Family
- PolyethylenesPolyolefins
Tasnee HD 100 Black is a High Density Polyethylene, black colored resin. The product is classified as PE 100. Tasnee HD 100 Black provides excellent environmental stress cracking resistance properties (ESCR) with very good long term hydrostatic strength and combines very high impact and stiffness properties.
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Agriculture & Feed — Agricultural Films
- Pipes & Hoses
Building & Construction — Building Materials
- Pipes & Plumbing
Product Families
Plastics — Basic Thermoplastics
- Polyolefins
Other characteristics
- Brand
- Tasnee HDPE
- Polymer Name
- High Density Polyethylene (HDPE)
- Melt Flow Index
- 0.23 - 0.23 g/10 min, 6.4 - 6.4 g/10 min
- Processing Methods
- Extrusion
- Color
- Black
- Markets
- Agriculture & Feed
- Building & Construction
- Technology
- Plastics
- Packaging Type
- Bags
- Material Features
Good Environmental Stress Crack Resistance (ESCR); Good Stiffness; High Impact Performance; Hydrostatic Strength; Odorless
- Plastics and Elastomers End Uses
- Pipes
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
Technical data
Table 1 of 2
20 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Charpy Notched Impact Strength (at -30°C) | 13 | kJ/m2 | ISO 179 |
| Charpy Notched Impact Strength (at 23°C) | 26 | kJ/m2 | ISO 179 |
| Flexural Stress (at 3,5% deflection) | 21 | MPa | ISO 178 |
| Injection Molding Melt Temperature | 200 - 280 | °C | — |
| Melt Temperature | 190 - 220 | °C | — |
| Odor Treshold | max. 2 | — | EN 1622 / EN 1240 |
| Oxidation Induction Time (OIT, 210°C) | 30 | minute | EN 728 |
| Shore Hardness (Shore D, 3 sec) | 63 | — | ISO 868 |
| Tensile Creep Modulus 1000h | 360 [2.0] | MPa | ISO 899-1 |
| Tensile Creep Modulus 1h | 850 [2.0] | MPa | ISO 899-1 |
| Tensile Modulus (at 23°C, v = 1mm/min, Secant) | 900 | MPa | ISO 527-1,-2 |
| Tensile Strain at Yield (at 23°C, v = 50 mm/min) | 9 | % | ISO 527-1,-2 |
Table 2 of 2
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 0.959 | g/cm3 | ISO 1183 |
| Melt Flow Rate (190°C / 21.6kg) | 6.4 | g/10 min | ISO 1133 |
| Melt Flow Rate (190°C / 5kg) | 0.23 | g / 10 min | ISO 1133 |
| Staudinger Index Jg | 380 | ml/g | ISO 1628 |
| Vicat Softening Temperature (VST/B/50 K/h (50N)) | 74 | °C | ISO 306 |