To catalogue
Crosslink Technologies XRD1018
- Chemical Family
- Epoxy & Epoxy Derivatives
Crosslink Technologies XRD1018 is a two component, room temperature cure semi-flexible, flame retardant, epoxy system. The system was developed for potting/casting of electrical and electronic components. its use of non-abrasive fillers and convenient 1 to 1 ratio by volume, make it ideal for use in machine dispensing equipment. This product meets ul94-v0 in house flammability testing.
Product families
Applications
Applications
- Electrical & Electronics — Other Electrical & Electronics Applications
Electrical & Electronics — Packaging & Assembly
- Potting Compounds
Product Families
Plastics — Thermoset Resins
- Epoxies
Other characteristics
- End Uses
Electrical Components, Electrical/Electronic Applications, Encapsulant, General Purpose
- Polymer Name
- Epoxy Resins & Compounds
- Processing Methods
- Casting, Potting
- Volume Resistivity
- 2000000000000.0 - 2000000000000.0 Ohm-m
- Markets
- Electrical & Electronics
- Shelf LIfe
- 12 Months
- Cure
- Air Dry
- Flame Rating
- UL 94 V0
- Technology
- Plastics
- Cure Schedule
- Recommended Cure Schedule at 22 °C - 24 Hrs
- Alternate Cure Schedule at 60 °C - 6 Hrs.
- Material Features
- Cost Effective
- Easier Processing
- Filled
- Flame Retardant
- General Purpose
- Improved Flexibility
- Certifications and Compliance
- UL 94
- Plastics and Elastomers End Uses
- Electrical Components
- Electrical/Electronic Applications
- Encapsulant
- General Purpose
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Casting
- Potting
Technical data
Table 1 of 4
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Viscosity | 8,000 - 15,000 | cps |
| Specific Gravity | 1.42 - 1.48 | g/cm³ |
Table 2 of 4
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Dielectric Constant at 1 KHz | 4.2 | — |
| Dissipation Factor at 1 KHz | 0.02 | — |
| Dielectric Strength (125 Mil/Section) | 380 | Volts/Mil |
| Volume Resistivity | 2.0 x10^14 | Ohm/Cm |
Table 3 of 4
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1.45 | gm/Cm³ | — |
| Hardness | 65 | Shore D | — |
| Tensile Strength | 1100 | Psi | Astm D 638 |
| Tensile Elongation | 50 | % | Astm D 638 |
| Coefficient of Thermal Expansion | 10X10^-6 | in/in/°C | — |
| Flammability | 0 | Cal/Sec.Cm.°C | — |
Table 4 of 4
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Mix Ratio By Weight (by vol. 100:100.0) | 100:100.0 | — |
| Mixed Viscosity at 22°C | 7500 | cps |
| Pot Life Of 200 gm. mass at 22°C | 30 | minutes |
| Gel Time Of 200 gm. mass at 22°C | 75 | hours |