To catalogue
Crosslink Technologies CLR1876
- Chemical Family
- Epoxy & Epoxy Derivatives
Crosslink Technologies CLR1876 is a thermally conductive, two part epoxy system. the system was secifically designed for applications where heat dissipation on thermally sensitive devices is required.
Product families
Applications
Applications
- Electrical & Electronics — Other Electrical & Electronics Applications
Electrical & Electronics — Packaging & Assembly
- Potting Compounds
Product Families
Plastics — Thermoset Resins
- Epoxies
Other characteristics
- End Uses
Electrical Components, Electrical/Electronic Applications, Encapsulant
- Polymer Name
- Epoxy Resins & Compounds
- Processing Methods
- Casting, Potting
- Volume Resistivity
- 200000000000000.0 - 200000000000000.0 Ohm-m
- Markets
- Electrical & Electronics
- Shelf LIfe
- 12 Months
- Cure
- Air Dry
- Technology
- Plastics
- Cure Schedule
- Recommended Cure Schedule at 22 °C - 24 Hrs
- Alternate Cure Schedule at 60 °C - 4 Hrs.
- Material Features
- Filled
- Thermally Conductive
- Plastics and Elastomers End Uses
- Electrical Components
- Electrical/Electronic Applications
- Encapsulant
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Casting
- Potting
Technical data
Table 1 of 4
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Viscosity | 50,000 - 100,000 | cps |
| Specific Gravity | 2.47 - 2.53 | g/cm³ |
Table 2 of 4
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Dielectric Constant at 1 KHz | 6.6 | — |
| Dissipation Factor at 1 KHz | 0.012 | — |
| Dielectric Strength (125 Mil/Section) | 500 | Volts/Mil |
| Volume Resistivity | 200 x10^14 | Ohm/Cm |
Table 3 of 4
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 2.4 | gm/Cm³ | — |
| Hardness | 90 | Shore D | — |
| Linear Shrinkage | 0.001 | In/In | Astm D 2566 |
| Tensile Strength | 8500 | Psi | Astm D 638 |
| Thermal Conductivity | 35X10^-4 | Cal/Sec.Cm.°C | — |
| Moisture Absorption | 0.1 | % | — |
| Flextural Strength | 14000 | Psi | — |
Table 4 of 4
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Mix Ratio By Weight (A:B) | 100:3.0 | — |
| Mixed Viscosity at 22°C | 37500 | cps |
| Pot Life Of 200 gm. mass at 22°C | 20 | minutes |
| Gel Time Of 200 gm. mass at 22°C | 45 | minutes |