To catalogue
Formac Elastomerised Formamid 6
- Chemical Family
- Polyamides
Formac Elastomerised Formamid 6 is used for automotive & farming mechanics, consumer goods and industrial applications. It has good mechanical resistance, elasticity and resistance to impact. Injection molding grade with good melt flowability.
Product families
Applications
Applications
- Consumer Goods — Appliances & Electronics; Consumer Goods — Lawn & Garden; Consumer Goods — Other Consumer Goods Applications; Consumer Goods — Sports & Recreation
Automotive & Transportation — Automotive
- Interior
- Other Automotive Applications
- Powertrain & UTH
Industrial — Chemical & Industrial Manufacturing
- Equipment & Parts
Product Families
Plastics — Engineering & Specialty Polymers
- Polyamides
Other characteristics
- Polymer Name
- Polyamide 6 (PA 6)
- Flexural Modulus
- 1750.0 - 1750.0 MPa
- Processing Methods
- Injection Molding
- Color
- Black
- Markets
- Automotive & Transportation
- Consumer Goods
- Industrial
- Flame Rating
- UL 94 HB
- Technology
- Plastics
- Material Features
- Good Impact Strength
- Good Mechanical Properties
- High Elasticity
- High Impact Resistance
- High Melt Flow
- Low Temperature Impact Resistance
- Certifications and Compliance
- ISO 9001
- UL 94
- Plastics and Elastomers End Uses
- Automotive Applications
- Automotive Interior Parts
- Automotive Under The Hood
- Consumer Applications
- Doors
- Industrial Parts
- Sporting Goods
- Windows
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 7
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Point (DSC) | 220.0 | °C | ISO 3146 |
Table 2 of 7
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 2100.0 | MPa | ISO 527 - 2 |
| Stress at Break | 48.0 | MPa | ISO 527 - 2 |
| Yield Strain | 4.3 | % | ISO 527 - 2 |
| Strain at Break | min. 50 | % | ISO 527 - 2 |
| Flexural Modulus | 1750.0 | MPa | ISO 178 |
| Maximum Flexural Stress | 70.0 | MPa | ISO 178 |
| IZOD Notched Impact Strength (+23°C) | 60.0 | KJ/m2 | ISO 180/1eA |
Table 3 of 7
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Heat Distortion Temperature (Under 1.8 Mpa Load, HDT A) | 60.0 | °C | ISO 75 - 2 |
| Heat Distortion Temperature (Under 0.45 MPa Load, HDT B) | 130.0 | °C | ISO 75 - 2 |
Table 4 of 7
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Volume Resistivity | 10000000000000.0 | Ω*cm | IEC 60093 |
| Surface Resistivity | 100000000000000.0 | Ω | IEC 60093 |
| Comparative Tracking Index | 500.0 | V | IEC 60112 |
| Oxigen Index | 20.0 | % | ISO 4589-1/-2 |
Table 5 of 7
3 rows| Characteristic | Value | Method |
|---|---|---|
| Flammability Rate (0.8 mm thickness) | HB | UL94 |
| Flammability Rate (1.6 mm thickness) | HB | UL94 |
| Flammability Rate (3.2 mm thickness) | HB | UL94 |
Table 6 of 7
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Temperature | 275-295 | °C | CYLINDER |
| Melt Mold | 70-80 | °C | MOLD |
| Drying Temperature | 80.0 | °C | — |
Table 7 of 7
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1.08 | g/cm3 | ISO 1183 |
| Humidity Absorption | 2.5 | % | Similar ISO 62 |
| Mould Shrinkage (Parallel) | 1.3 | % | ISO 2577 |
| Mould Shrinkage (Normal) | 1.55 | % | ISO 2577 |