WIC PP 15 BK is a polypropylene base polymer filled with 15% carbon fiber and colored black. Its processing conditions involve injection molding with a melt temperature of 210-260°C and a mold temperature of 30-60°C. It has special features such as heat aging stabilization and is suitable for the Automotive and Sport market segments. Under certain conditions, the increased thermal conductivity needs to be considered.
Product families
Plastics — Basic Thermoplastics
- Polyolefins
Other characteristics
- Brand
- WIC
- Polymer Name
- Polypropylene Copolymer
- Fillers Included
- Carbon Fiber
- Processing Methods
- Injection Molding
- Color
- Black
- Markets
- Consumer Goods
- Applications
- Consumer Goods — Sports & Recreation
- Technology
- Plastics
- Labeling Claims
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Material Features
- Heat Aging Resistant
- Storage Condition
- Store in dry, protected from light.
- Pre-Drying Conditions
- 80°C in an air circulating dryer for 2-4h
- Dependant on moisture content
- Certifications and Compliance
- IATF 16949
- ISO 13485
- ISO 14001
- ISO 17025
- ISO 45001
- ISO 50001
- ISO 9001
- RoHS Compliant
- Plastics and Elastomers End Uses
- Automotive Applications
- Sporting Goods
- Plastics and Elastomers Functions
- Resin
- Injection Moulding Processing Conditions
Under certain conditions the increased thermal conductivity must be considered.
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 6
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 8000.0 | MPa | ISO 527 |
| Tensile Strength | 72.0 | MPa | ISO 527 |
| Tensile Elongation at Yield | 2.0 | % | ISO 527 |
| Tensile Strength at Break | 75.0 | MPa | ISO 527 |
| Tensile Elongation at Break | 4.0 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | 40.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Charpy, at 23°C) | 8.0 | kJ/m² | ISO 179/1eA |
Table 2 of 6
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 990.0 | kg/m³ | ISO 1183 |
| Global Warming Potential (GWP) | 1.42 | kg CO₂ eq. | ISO 14040, 14044 |
Table 3 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Vicat B50 | 115.0 | °C | ISO 306 |
| HDT / A (1.8 MPa) | 150.0 | °C | ISO 75-1/-2 |
| DSC (Melt Point) | 160.0 | °C | ISO 11357-1/-3 |
Table 4 of 6
1 row| Characteristic | Value | Unit |
|---|---|---|
| Moisture Content | max. 0.1 | % |
Table 5 of 6
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Melt Temperature | 210 - 260 | °C |
| Mould Temperature | 30 - 60 | °C |
Table 6 of 6
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Index (MVR) | 17.0 | cm³/10min | ISO 1133 |
| MVR Temperature | 230.0 | °C | — |
| MVR Load | 2.16 | kg | — |
| Molding Shrinkage (parallel) | 0.4 | % | ISO 294-4, 2577 |
| Molding Shrinkage (normal) | 0.4 | % | ISO 294-4, 2577 |