To catalogue

POLYSLICK FENDER PADS

POLYSLICK FENDER PADS fender facings bolted or bonded to a fender front creates an unbreakable, low friction shield which protects surfaces from impact and abrasion. UHMW can be designed into the construction of new fendering structures, enduring continuous impact and rubbing, prolonged ultra violet light exposure, wide temperature variations, salt and chemical contact. UHMW fenders can be made of UHMW, crosslinked UHMW, or reprocessed UHMW. Our Custom Fenders can be fabricated, heat or cold formed to customer specifications.

Properties

Physical Form
Custom

Product families

Automotive & Transportation — Transportation
  • Marine

Other characteristics

Brand
POLYSLICK
Density
932.0 - 932.0 kg/m³
Features

Abrasion Resistant, Good UV Protection, Impact Resistance, Non Corrosive

Polymer Name

Ultra High Molecular Weight Polyethylene (UHMWPE)

Markets
Automotive & Transportation
Key Features

Impact resistant.; Abrasion resistant.; UV protected.; Will not corrode, rot or splinter.; Resists marine borers and barnacle growth.; Non-sparking.; Can be drilled, chamfered and fabricated to meet customer specifications.

Technology
Plastics
Product Families
Plastics — Parts, Shapes & Films
Material Features
  • Abrasion Resistant
  • Good UV Protection
  • Impact Resistance
  • Non Corrosive
Recommended Applications
  • Dock Facings.
  • Bridge Fenders.
  • Boat Rails and Gunnels.
  • Canal Lock Door Panels.
  • Lock and Dam Guidewall.
  • Dry Dock Walls and Side Rails.
  • Floating Docks.
  • Pipeline Fenders.
Plastics and Elastomers End Uses
Fenders

Technical data

Table 1 of 3

3 rows
CharacteristicValueUnitMethod
Melting Point271°F—
Coef. Of Linear Thermal Expansion8.3 X 10^-5in/in/°FASTM-D696
FlammabilityHB (1/8 inch)—UL-94

Table 2 of 3

9 rows
CharacteristicValueUnitMethod
Abrasion Resistance10——
Coefficient of Friction, Kinetic0.15—UL410
Coefficient of Friction, Static0.2—UL410
Density0.932g/ccASTM-D792
Durometer Hardness64Shore DASTM-D2240
Elongation at Break300%ASTM-D638
Izod Impact Srengthmin. 100KJ/m2ASTM-D4020, Method A
Tensile Strength at Yield3500psiASTM-D638
Water Absorbtion at Saturation0.01%ASTM-D570

Table 3 of 3

4 rows
CharacteristicValueUnitMethod
Dielectric Constant2.3—ASTM-D150
Dielectric Strength90.3KV/mASTM-D149
Surface Resistivity1 X 10^12ohmASTM-D257
Volume Resistivity1 X 10^14ohm-cmASTM-D257

The Omnichem website uses cookies. By continuing to use the site, you consent to their use in accordance with our Privacy Policy and to the collection of analytics.