AVALANCHE HIGH TEMP LINERS
- Chemical Family
- PolyethylenesPolyolefins
AVALANCHE HIGH TEMP LINERS are designed to haul hot asphalt up to a temperature of 400 degrees Fahrenheit. Our Heat Stabilized dump truck liner is our most durable & protective liner, while also utilizing additives to provide for our best sliding surface to fight against material build up and additional hydraulic pressure used to extract material from your dump truck bed. When compared to HMW liners, UHMW liners are 3-5X more resistant to wear. The High Temperature liner ranges from 1/4” to 1/2” thickness, and can be manufactured in widths from 1’ to 16’ feet wide.
Properties
- Physical Form
- Film
Product families
- Structural Components
- Commercial
Other characteristics
- Brand
- AVALANCHE
- Density
- 935.0 - 935.0 kg/m³
- Features
Excellent Water Resistance, Good Sliding Properties, Good UV Protection, Lubricated
- Polymer Name
Ultra High Molecular Weight Polyethylene (UHMWPE)
- Markets
- Automotive & Transportation
- Building & Construction
- Key Features
Specially formulated UHMW-PE for temperatures up to 400ºF.; Toughest liner for hot asphalt.; Best sliding surface.; Lifetime warranty available.; UV protection.; Reduces haulback.; Added lubricity.; Added water protection.; Eliminates freezing
- Technology
- Plastics
- Product Families
- Plastics — Parts, Shapes & Films
- Material Features
- Excellent Water Resistance
- Good Sliding Properties
- Good UV Protection
- Lubricated
- Recommended Applications
- Hopper Liners.
- Blacktop Liners.
- Gravity Box Liners.
- Dump Truck Liners.
- Forage Box Liners.
- Forage Wagon Liners.
- Manure Spreader Liners.
- Air Boat Hull Bottom Liners.
- Plastics and Elastomers End Uses
- Bed Liners
- Truck Liners
Technical data
Table 1 of 3
9 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Abrasion Resistance | 9 | — | — |
| Coefficient of Friction, Kinetic | 0.1 | — | ASTM-D1894 |
| Coefficient of Friction, Static | 0.15 | — | ASTM-D1894 |
| Density | 0.935 | g/cc | ASTM-D792 |
| Durometer Hardness | 64 | Shore D | ASTM-D2240 |
| Elongation at Break | 250 | % | ASTM-D638 |
| Izod Impact Srength | min. 95 | KJ/m2 | ASTM-D4020, Method A |
| Tensile Strength at Yield | 3100 | psi | ASTM-D638 |
| Water Absorbtion at Saturation | 0.01 | % | ASTM-D570 |
Table 2 of 3
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Point | min. 350 | °F | — |
| Coef. Of Linear Thermal Expansion | 7 X 10^-6 | in/in/°F | ASTM-D696 |
| Flammability | HB (1/8 inch) | — | UL-94 |
Table 3 of 3
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Dielectric Constant | 2.3 | — | ASTM-D150 |
| Dielectric Strength | 90.3 | KV/m | ASTM-D149 |
| Surface Resistivity | 1 X 10^12 | ohm | ASTM-D257 |
| Volume Resistivity | 1 X 10^14 | ohm-cm | ASTM-D257 |