ALCOM® MS ECO PC+ABS R 1000 SL
MOCOM Compounds ALCOM® MS ECO PC+ABS R 1000 SL is an injection molding grade modified for antisqueak properties, containing recycled material and providing easy release for demolding. Mainly used in the automotive industry for interior decoration and finishing, such as housings, the melt temperature for injection molding is 240-250°C and the mold temperature should be 70-100°C.
Product families
Applications
- Housings & Enclosures
Product Families
- Blends & Alloys
Other characteristics
- Brand
- ALCOM
- Density
- 1120.0 - 1120.0 kg/m³
- Polymer Name
- PC/ABS Alloy
- Flexural Modulus
- 2200.0 - 2200.0 MPa
- Processing Methods
- Injection Molding
- Markets
- Electrical & Electronics
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Conflict minerals-free
- PAH-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Recycled
- Additives Included
- Anti-Squeak Agent
- Material Features
- Anti-Squeaking
- Good Mold Release
- Storage Condition
- Store in dry, protected from light.
- Pre-Drying Conditions
100-110 °C in a dry air (dessiccant) dryer for 2-4 h; In an air circulatIng dryer 100-110 °C for 3-6 h
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers End Uses
- Automotive Applications
- Housings
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 5
11 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Modulus | 2200.0 | MPa | ISO 178 |
| Flexural Stress (3.5% Strain) | 65.0 | MPa | ISO 178 |
| Tensile Modulus | 2000.0 | MPa | ISO 527 |
| Tensile Stress at Yield | 45.0 | MPa | ISO 527 |
| Tensile Elongation at Yield | 3.3 | % | ISO 527 |
| Tensile Elongation at Break | 40.0 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | no break | kJ/m² | ISO 179/1eU |
| Impact Strength (Charpy, at -40°C) | 240.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Charpy, at 23°C) | 50.0 | kJ/m² | ISO 179/1eA |
| Notched Impact (Charpy, at -40°C) | 10.0 | kJ/m² | ISO 179/1eA |
| Ball Indentation Hardness (H358/30) | 90.0 | MPa | ISO 2039-1 |
Table 2 of 5
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1120.0 | kg/m³ | ISO 1183 |
Table 3 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Vicat B50 | 108.0 | °C | ISO 306 |
| HDT / A (1.8 MPa) | 98.0 | °C | ISO 75-1/-2 |
Table 4 of 5
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Melt Temperature | 240 - 250 | °C |
| Mould Temperature | 70 - 100 | °C |
Table 5 of 5
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Index (MVR) | 20.0 | cm³/10min | ISO 1133 |
| MVR Temperature | 260.0 | °C | — |
| MVR Load | 5.0 | kg | — |
| Shrinkage (24h) | 0.6 - 0.9 | % | ISO 294-4 |