To catalogue

ALTECH® MBS A 1000/500

CAS Number
25322-68-3
Chemical Family
Styrenics

MOCOM Compounds ALTECH® MBS A 1000/500 is a polystyrene copolymer that is processing stabilized, elastomer modified, and injection molding grade. When used for injection molding, the melt temperature should range from 190-230°C and the mold temperature should range from 10-60°C. This product is suitable for various applications and provides excellent results.

Product families

Elastomers — Thermoplastic Elastomers
  • Styrenic Thermoplastic Elastomers (TPE-S)

Other characteristics

Brand
ALTECH
Polymer Name
Methyl Methacrylate Butadiene Styrene (MBS)
Labeling Claims

Azo Colorants-free, Azo Dyes-free, Conflict minerals-free, PAH-free, PFOA-free, PFOS-free, Persistent Organic Pollutants (POP)-free; Azo Colorants-free; Azo Dyes-free; Conflict minerals-free; PAH-free; PFOA-free; PFOS-free; Persistent Organic Pollutants (POP)-free

Strain at Break
45.0 - 45.0 %
Additives Included
Processing Stabilizer
Processing Methods
Injection Molding
Certifications & Compliance

Directive 2011/65/EC amended through EU/2015/863 (RoHS), EC No.1907/2006, IATF 16949, ISO 13485, ISO 14001, ISO 17025, ISO 45001, ISO 50001, ISO 9001, REACH (Europe), REACH (UK), RoHS Compliant, SVHC Compliant

Technology
Elastomers
Material Features
  • Elastomer Modified
  • Processing Stability
Storage Condition
Store in dry, protected from light.
Pre-Drying Conditions
65 °C in a dry air (dessiccant) dryer for 2-3 h
Certifications and Compliance

Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant

Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 6

11 rows
CharacteristicValueUnitMethod
Flexural Modulus2050.0MPaISO 178
Flexural Stress (3.5% Strain)43.0MPaISO 178
Tensile Modulus2000.0MPaISO 527
Tensile Stress at Yield26.0MPaISO 527
Tensile Elongation at Yield2.0%ISO 527
Tensile Elongation at Break45.0%ISO 527
Impact Strength (Charpy, at 23°C)75.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)20.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)6.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)1.5kJ/m²ISO 179/1eA
Ball Indentation Hardness (H132/30)60.0MPaISO 2039-1

Table 2 of 6

1 row
CharacteristicValueUnitMethod
Density1040.0kg/m³ISO 1183

Table 3 of 6

2 rows
CharacteristicValueUnitMethod
Vicat B5070.0°CISO 306
HDT / A (1.8 MPa)71.0°CISO 75-1/-2

Table 4 of 6

4 rows
CharacteristicValueUnitMethod
Flammability (1.5 mm)HBclassUL 94
Flammability (3.0 mm)HBclassUL 94
Glow Wire (GWFI, 650°C, 1mm)Passed—DIN EN 60695
Glow Wire (GWFI, 650°C, 2mm)Passed—DIN EN 60695

Table 5 of 6

2 rows
CharacteristicValueUnit
Mould Temperature10 - 60°C
Melt Temperature190 - 230°C

Table 6 of 6

4 rows
CharacteristicValueUnitMethod
Melt Index (MVR)55.0cm³/10minISO 1133
MVR Temperature220.0°C—
MVR Load10.0kg—
Shrinkage (24h)0.4 - 0.8%ISO 294-4