TEDUR® L 9300-1
- Chemical Family
- Polyphenylene Sulfide (PPS)
MOCOM Compounds TEDUR® L 9300-1 is a Polyphenylene Sulfide base polymer with 40% glass fibers/glass beads filler/additive system, colored black. It has high toughness, reduced flash, increased burst strength, and low warpage, making it suitable for various applications. To ensure optimal performance, TEDUR® L 9300-1 should be protected from light and stored at a temperature not exceeding 30°C. For injection molding, a melt temperature of 320-340°C and a mold temperature greater than 140°C is recommended.
Product families
- High Performance Thermoplastics
Other characteristics
- Brand
- TEDUR
- Polymer Name
- Polyphenylene Sulfide (PPS)
- Fillers Included
- Glass Bead, Glass Bead/Glass Fiber
- Glass Bead
- Glass Bead/Glass Fiber
- Flexural Modulus
- 13000.0 - 13000.0 MPa
- Processing Methods
- Injection Molding
- Color
- Black
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Conflict minerals-free
- PAH-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Material Features
- Excellent Toughness
- Good Flow
- High Temperature Resistance
- Increased Burst Strength
- Low Flash
- Low Warpage
- Storage Condition
Store in dry, protected from light not above 30°C.
- Pre-Drying Conditions
In a dry air (dessiccant) dryer 130-140 °C for 2-4 h; Dependant on moisture content
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 5
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Modulus | 13000.0 | MPa | ISO 178 |
| Flexural Strength | 250.0 | MPa | ISO 178 |
| Tensile Modulus | 13500.0 | MPa | ISO 527 |
| Flexural Deflection (Maximum Force) | 2.0 | % | ISO 178 |
| Tensile Strength at Break | 170.0 | MPa | ISO 527 |
| Tensile Elongation at Break | 1.8 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | 44.0 | kJ/m² | ISO 179/1eU |
Table 2 of 5
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1650.0 | kg/m³ | ISO 1183 |
Table 3 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| HDT / A (1.8 MPa) | 270.0 | °C | ISO 75-1/-2 |
| DSC (Melt Point) | 280.0 | °C | ISO 11357 |
Table 4 of 5
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flammability (0.75 m) | V - 0 | class | UL 94 |
| UL Recognition | yes | — | — |
| Glow Wire (GWFI, 960°C, 2mm) | Passed | — | DIN EN 60695 |
Table 5 of 5
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Mould Temperature | min. 140 | °C |
| Melt Temperature | 320 - 340 | °C |