ALTECH® ECO PP-H 2030/W100.05 BK0002
- Chemical Family
- PolyolefinsPolypropylenes (PP)
MOCOM Compounds ALTECH® ECO PP-H 2030/W100.05 BK0002 is a polypropylene homopolymer with 30% glass fiber filled, black in color and pre-dried at 80-100°C in an air circulating dryer for 2-4 hours, depending on moisture content with a maximum moisture content of 0.10%. It is suitable for injection molding with a melt temperature of 200-270°C and mold temperature of 20-60°C, and is processing stabilized for Automotive and Various market segments. For optimal performance, it should be stored in a dry and light-protected area to maximize its effectiveness.
Product families
- Polyolefins
Other characteristics
- Brand
- ALTECH® ECO
- Polymer Name
- Polypropylene Homopolymer (HPP)
- Fillers Included
- Glass Fiber
- Additives Included
- Processing Stabilizer
- Processing Methods
- Injection Molding
- Color
- Black
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Conflict minerals-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Material Features
- Processing Stability
- Storage Condition
- Store in dry, protected from light.
- Pre-Drying Conditions
- 80-100°C in an air circulating dryer for 2-4h
- Dependant on moisture content
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers End Uses
- Automotive Applications
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 6
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 6000.0 | MPa | ISO 527 |
| Tensile Strength | 70.0 | MPa | ISO 527 |
| Tensile Elongation at Break | 3.0 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | 40.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Charpy, at 23°C) | 9.0 | kJ/m² | ISO 179/1eA |
Table 2 of 6
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1120.0 | kg/m³ | ISO 1183 |
| Global Warming Potential (GWP) | 1.31 | kg CO₂ eq. | ISO 14040, 14044 |
Table 3 of 6
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| HDT / B (0.45 MPa) | 161.0 | °C | ISO 75-1/-2 |
Table 4 of 6
1 row| Characteristic | Value | Unit |
|---|---|---|
| Moisture Content | max. 0.1 | % |
Table 5 of 6
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Mould Temperature | 20 - 60 | °C |
| Melt Temperature | 200 - 270 | °C |
Table 6 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Index (MVR) | 10.0 | cm³/10min | ISO 1133 |
| MVR Temperature | 230.0 | °C | — |
| MVR Load | 2.16 | kg | — |