ALCOM® ASA 540/7 UV SV1281-08MCF
- Chemical Family
- Styrenics
MOCOM Compounds ALCOM® ASA 540/7 UV SV1281-08MCF is a UV-stabilized Acrylonitile/Styrene/Acrylate/Copolymer with a low tendency to form flow lines and a metallic effect, similar to that of RAL 9006. It is suitable for injection molding with a melt temperature range of 240-280°C, and a mold temperature range of 40-80°C. It is suitable for use in electrical and electronic, building and construction, and sport and leisure applications, such as for housings. For optimal performance, it should be stored in a dry and light-protected environment.
Product families
Applications
- Consumer Goods — Sports & Recreation
- Housings & Enclosures
Product Families
- Styrenics
Other characteristics
- Brand
- ALCOM
- Polymer Name
- Acrylonitrile Styrene Acrylate (ASA)
- Additives Included
- UV Stabilizer
- Processing Methods
- Injection Molding
- Markets
- Consumer Goods
- Electrical & Electronics
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Conflict minerals-free
- PAH-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Material Features
- UV Resistant
- UV Stabilized
- Storage Condition
- Store in dry, protected from light.
- Pre-Drying Conditions
- 80 °C in a dry air (dessiccant) dryer for 2-4 h
- 80 °C in an air circulating dryer for 3-6 h
- Dependant on moisture content
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers End Uses
- Construction Applications
- Electrical/Electronic Applications
- Housings
- Sporting Goods
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 5
11 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Modulus | 2900.0 | MPa | ISO 178 |
| Flexural Stress (3.5% Strain) | 74.0 | MPa | ISO 178 |
| Tensile Modulus | 2700.0 | MPa | ISO 527 |
| Tensile Stress at Yield | 49.0 | MPa | ISO 527 |
| Tensile Elongation at Yield | 3.1 | % | ISO 527 |
| Tensile Elongation at Break | 6.3 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | 35.0 | kJ/m² | ISO 179/1eU |
| Impact Strength (Charpy, at -40°C) | 15.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Charpy, at 23°C) | 8.0 | kJ/m² | ISO 179/1eA |
| Notched Impact (Charpy, at -40°C) | 2.0 | kJ/m² | ISO 179/1eA |
| Ball Indentation Hardness (H358/30) | 97.0 | MPa | ISO 2039-1 |
Table 2 of 5
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1120.0 | kg/m³ | ISO 1183 |
Table 3 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Vicat B50 | 101.0 | °C | ISO 306 |
| HDT / A (1.8 MPa) | 92.0 | °C | ISO 75-1/-2 |
Table 4 of 5
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Melt Temperature | 240 - 280 | °C |
| Mould Temperature | 40 - 80 | °C |
Table 5 of 5
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Index (MVR) | 6.0 | cm³/10min | ISO 1133 |
| MVR Temperature | 220.0 | °C | — |
| MVR Load | 10.0 | kg | — |
| Shrinkage (24h) | 0.4 - 0.7 | % | ISO 294-4 |