ALCOM® PA66 910/1.1 CF10 IM
- Chemical Family
- Polyamides
MOCOM Compounds ALCOM® PA66 910/1.1 CF10 IM is a Polyamide 66 base polymer with 10% carbon fibers, and it is designed for applications in the Automotive and Machinery markets, such as injection molded parts like bearings and sliding elements and functional components. It has special features including electrically conductive, reduced surface resistivity, impact modified, and heat stabilized.
Product families
- Polyamides
Other characteristics
- Brand
- ALCOM
- Polymer Name
- Polyamide 66 (PA 66)
- Fillers Included
- Carbon Fiber
- Additives Included
- Heat Stabilizer, Impact Modifier
- Heat Stabilizer
- Impact Modifier
- Processing Methods
- Injection Molding
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Conflict minerals-free
- PAH-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Material Features
- Electrically Conductive
- Heat Stabilized
- Impact Modified
- Reduced Surface Resistivity
- Storage Condition
- Store in dry, protected from light.
- Pre-Drying Conditions
- 80 °C in a dry air (dessiccant) dryer for 2-12 h
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers End Uses
- Automotive Applications
- Bearings
- Machine/Mechanical Parts
- Sliding Parts
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 7
9 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Modulus (Dry) | 7400.0 | MPa | ISO 178 |
| Flexural Strength (Dry) | 215.0 | MPa | ISO 178 |
| Tensile Modulus (Dry) | 8900.0 | MPa | ISO 527 |
| Tensile Strength at Break (Dry) | 155.0 | MPa | ISO 527 |
| Tensile Elongation at Break (Dry) | 2.8 | % | ISO 527 |
| Impact Strength (Dry, Charpy, at 23°C) | 45.0 | kJ/m² | ISO 179/1eU |
| Impact Strength (Dry, Charpy, at -40°C) | 30.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Dry, Charpy, at 23°C) | 5.0 | kJ/m² | ISO 179/1eA |
| Notched Impact (Dry, Charpy, at -40°C) | 3.5 | kJ/m² | ISO 179/1eA |
Table 2 of 7
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density (Dry) | 1170.0 | kg/m³ | ISO 1183 |
Table 3 of 7
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| HDT / A (Dry, 1.8 MPa) | 250.0 | °C | ISO 75-1/-2 |
| DSC (Melt Point, Dry) | 263.0 | °C | ISO 11357 |
Table 4 of 7
1 row| Characteristic | Value | Unit |
|---|---|---|
| Moisture Content | max. 0.15 | % |
Table 5 of 7
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Surface Resistance (Conditioned) | max. 500 | Ohm | IEC 62631-3-2 |
Table 6 of 7
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Melt Temperature | 280 - 300 | °C |
| Mould Temperature | 80 - 120 | °C |
Table 7 of 7
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Shrinkage (Lengthwise, 24h) | 0.1 - 0.3 | % | ISO 294-4 |
| Shrinkage (Lateral, 24h) | 0.6 - 0.8 | % | ISO 294-4 |