To catalogue

ALCOM® PP 620/1 WT1034-05LB

MOCOM Compounds ALCOM® PP 620/1 WT1034-05LB is a base polymer of Polypropylene Homopolymer with a filler/additive system of 15% special filler and 15% mineral. It is highly reflective and opaque, making it suitable for applications such as light guides and reflectors, and is used in the automotive and lighting market segment. The pre-drying conditions involve being in a dry air (dessiccant) dryer or air circulating dryer set between 80-100°C for 2-4 hours with a maximum moisture content of <0.02%. The processing injection molding requires a melt temperature of 230-270°C and a mold temperature of 20-90°C.

Product families

Applications

Automotive & Transportation — Automotive
  • Aftermarket Parts & Components
  • Automotive Lighting
  • Exterior & Body

Product Families

Plastics — Basic Thermoplastics
  • Polyolefins

Other characteristics

Brand
ALCOM
Functions
Resin
Polymer Name
Polypropylene Homopolymer (HPP)
Labeling Claims

Azo Colorants-free, Azo Dyes-free, Conflict minerals-free, PAH-free, PFOA-free, PFOS-free, Persistent Organic Pollutants (POP)-free; Azo Colorants-free; Azo Dyes-free; Conflict minerals-free; PAH-free; PFOA-free; PFOS-free; Persistent Organic Pollutants (POP)-free

Fillers Included
  • Mineral, Proprietary
  • Mineral
  • Proprietary
Processing Methods
Injection Molding
Certifications & Compliance

Directive 2011/65/EC amended through EU/2015/863 (RoHS), EC No.1907/2006, IATF 16949, ISO 13485, ISO 14001, ISO 17025, ISO 45001, ISO 50001, ISO 9001, REACH (Europe), REACH (UK), RoHS Compliant, SVHC Compliant

Color
White
Markets
Automotive & Transportation
Technology
Plastics
Material Features
  • Excellent Opacity
  • Good Light Reflection
  • Heat Aging Resistant
  • High Reflectivity
  • Light Blocking
Storage Condition
Store in dry, protected from light.
Pre-Drying Conditions

In a dry air (dessiccant) dryer 80-100 °C for 2-3 h; In an air circulatIng dryer 80-100 °C for 2-4 h

Certifications and Compliance

Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant

Plastics and Elastomers End Uses
  • Automotive Applications
  • Automotive Exterior Parts
  • LED Housing
  • Light Blocking Components
  • Light Guides
  • Reflectors
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 7

10 rows
CharacteristicValueUnitMethod
Flexural Modulus2800.0MPaISO 178
Flexural Stress (3.5% Strain)47.0MPaISO 178
Tensile Modulus3100.0MPaISO 527
Tensile Stress at Yield31.0MPaISO 527
Tensile Elongation at Yield4.2%ISO 527
Tensile Elongation at Break9.5%ISO 527
Impact Strength (Charpy, at 23°C)40.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)13.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)2.5kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)1.5kJ/m²ISO 179/1eA

Table 2 of 7

1 row
CharacteristicValueUnitMethod
Density1160.0kg/m³ISO 1183

Table 3 of 7

3 rows
CharacteristicValueUnitMethod
Vicat B50101.0°CISO 306
HDT / A (1.8 MPa)79.0°CISO 75-1/-2
DSC (Melt Point)167.0°CISO 11357

Table 4 of 7

1 row
CharacteristicValueUnit
Moisture Contentmax. 0.02%

Table 5 of 7

2 rows
CharacteristicValueUnitMethod
Tristimulus Value Y10 of Reflection92.0%DIN 5033
Tristimulus Value Y10 of Transm.,d=0.5mm0.4%ISO 13468

Table 6 of 7

2 rows
CharacteristicValueUnit
Mould Temperature20 - 90°C
Melt Temperature230 - 270°C

Table 7 of 7

5 rows
CharacteristicValueUnitMethod
Melt Index (MVR)25.0cm³/10minISO 1133
MVR Temperature230.0°C—
MVR Load2.16kg—
Shrinkage (Lengthwise, 24h)1.2 - 1.7%ISO 294-4
Shrinkage (Lateral, 24h)0.9 - 1.4%ISO 294-4

The Omnichem website uses cookies. By continuing to use the site, you consent to their use in accordance with our Privacy Policy and to the collection of analytics.