ALCOM® ABS+SAN A 1000/100 SV2067-06MCF
MOCOM Compounds ALCOM® ABS+SAN A 1000/100 SV2067-06MCF has pre-drying conditions of 80°C in a dry air (dessiccant) dryer for 2-4 hours and 80°C in an air circulating dryer for 3-6 hours. Its base polymer is Acrylonitrile/butadiene/styrene + Styrene/acrylonitrile, and it has a metallic effect color. It has low tendency to flow lines and is used in the market segments of electrical and electronic, building and construction, and various. Its application area is for housings, fixing elements, and various, and it is processed by injection molding with a melt temperature of 220-260°C and mold temperature of 50-80°C. It should be stored in a dry and light-protected environment not exceeding 30°C.
Product families
Applications
- Interior Fixtures
- Housings & Enclosures
Product Families
- Blends & Alloys
Other characteristics
- Brand
- ALCOM
- Density
- 1080.0 - 1080.0 kg/m³
- Polymer Name
- ABS/SAN Alloy
- Flexural Modulus
- 2500.0 - 2500.0 MPa
- Processing Methods
- Injection Molding
- Markets
- Building & Construction
- Electrical & Electronics
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Conflict minerals-free
- PAH-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Storage Condition
Store in dry, protected from light not above 30°C.
- Pre-Drying Conditions
- 80 °C in a dry air (dessiccant) dryer for 2-4 h
- 80 °C in an air circulating dryer for 3-6 h
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers End Uses
- Construction Applications
- Electrical/Electronic Applications
- Fixtures
- Housings
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 5
11 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Modulus | 2500.0 | MPa | ISO 178 |
| Flexural Stress (3.5% Strain) | 70.0 | MPa | ISO 178 |
| Tensile Modulus | 2300.0 | MPa | ISO 527 |
| Tensile Stress at Yield | 44.0 | MPa | ISO 527 |
| Tensile Elongation at Yield | 2.5 | % | ISO 527 |
| Tensile Elongation at Break | 16.0 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | 110.0 | kJ/m² | ISO 179/1eU |
| Impact Strength (Charpy, at -40°C) | 75.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Charpy, at 23°C) | 22.0 | kJ/m² | ISO 179/1eA |
| Notched Impact (Charpy, at -40°C) | 7.5 | kJ/m² | ISO 179/1eA |
| Ball Indentation Hardness (H358/30) | 107.0 | MPa | ISO 2039-1 |
Table 2 of 5
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1080.0 | kg/m³ | ISO 1183 |
Table 3 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Vicat B50 | 100.0 | °C | ISO 306 |
| HDT / A (1.8 MPa) | 82.0 | °C | ISO 75-1/-2 |
Table 4 of 5
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Melt Temperature | 220 - 260 | °C |
| Mould Temperature | 50 - 80 | °C |
Table 5 of 5
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Index (MVR) | 11.0 | cm³/10min | ISO 1133 |
| MVR Temperature | 220.0 | °C | — |