ALCOM® ABS 530/22 SV1287-04MCS
- Chemical Family
- Acrylonitrile Butadiene Styrene (ABS)Styrenics
MOCOM Compounds ALCOM® ABS 530/22 SV1287-04MCS is a Base Polymer of Acrylonitrile/Butadiene/Styrene/Copolymer with a metallic effect color. It has good flow and is typically used to make housings for domestic appliances. Pre-drying Conditions include 80°C in an air circulating dryer for 3-6 hours and 80°C in a dry air (dessiccant) dryer for 2-4 hours depending on moisture content. For processing Injection molding, the melt temperature should be between 220-260°C and the mold temperature should be between 50-80°C.
Product families
Applications
- Consumer Goods — Appliances & Electronics
- Consumer Electronics
- Housings & Enclosures
Product Families
- Styrenics
Other characteristics
- Brand
- ALCOM
- Polymer Name
- Acrylonitrile Butadiene Styrene (ABS)
- Processing Methods
- Injection Molding
- Markets
- Consumer Goods
- Electrical & Electronics
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Conflict minerals-free
- PAH-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Material Features
- Good Flow
- Storage Condition
Store in dry, protected from light not above 30°C.
- Pre-Drying Conditions
- 80 °C in a dry air (dessiccant) dryer for 2-4 h
- 80 °C in an air circulating dryer for 3-6 h
- Dependant on moisture content
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers End Uses
- Appliances
- Housings
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 5
11 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Modulus | 2600.0 | MPa | ISO 178 |
| Flexural Stress (3.5% Strain) | 66.0 | MPa | ISO 178 |
| Tensile Modulus | 2300.0 | MPa | ISO 527 |
| Tensile Stress at Yield | 43.0 | MPa | ISO 527 |
| Tensile Elongation at Yield | 2.3 | % | ISO 527 |
| Tensile Elongation at Break | 12.0 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | 48.0 | kJ/m² | ISO 179/1eU |
| Impact Strength (Charpy, at -40°C) | 43.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Charpy, at 23°C) | 13.0 | kJ/m² | ISO 179/1eA |
| Notched Impact (Charpy, at -40°C) | 5.0 | kJ/m² | ISO 179/1eA |
| Ball Indentation Hardness (H358/30) | 100.0 | MPa | ISO 2039-1 |
Table 2 of 5
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1050.0 | kg/m³ | ISO 1183 |
Table 3 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Vicat B50 | 96.0 | °C | ISO 306 |
| HDT / A (1.8 MPa) | 85.0 | °C | ISO 75-1/-2 |
Table 4 of 5
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Melt Temperature | 220 - 260 | °C |
| Mould Temperature | 50 - 80 | °C |
Table 5 of 5
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Index (MVR) | 16.0 | cm³/10min | ISO 1133 |
| MVR Temperature | 220.0 | °C | — |
| MVR Load | 10.0 | kg | — |
| Shrinkage (24h) | 0.5 - 0.8 | % | ISO 294-4 |