To catalogue
CELLIDOR® B 631-12,5
- Chemical Family
- Cellulose & Cellulosics
MOCOM Compounds CELLIDOR® B 631-12,5 is a cellulose acetate butyrate polymer with a phthalate-free plasticiser system of 12-13%, a light stabilizer, and added features of high toughness, high surface quality, high surface gloss, good haptics, and good weathering resistance. It is used for extruded parts and profiles.
Product families
Plastics — Basic Thermoplastics
- Cellulosics
Other characteristics
- Brand
- CELLIDOR
- Density
- 1180.0 - 1180.0 kg/m³
- End Uses
- Profiles
- Polymer Name
- Cellulose Acetate Butyrate (CAB)
- Additives Included
- Light Stabilizer, Plasticizer (Phthalate-free)
- Light Stabilizer
- Plasticizer (Phthalate-free)
- Technology
- Plastics
- Labeling Claims
- Azo Colorants-free
- Azo Dyes-free
- Bio-based
- Conflict minerals-free
- PAH-free
- PFOA-free
- PFOS-free
- Persistent Organic Pollutants (POP)-free
- Material Features
- Excellent Toughness
- Good Haptics
- Good Surface Gloss
- Good Weather Stability
- Light Stabilized
- Non Phthalate Plasticizer
- Superior Surface Quality
- UV Resistant
- Storage Condition
- Store in dry, protected from light.
- Pre-Drying Conditions
- In an air circulatIng dryer 60-90 °C for 2-4 h
- Dependant on moisture content
- Certifications and Compliance
Directive 2011/65/EC amended through EU/2015/863 (RoHS); EC No.1907/2006; IATF 16949; ISO 13485; ISO 14001; ISO 17025; ISO 45001; ISO 50001; ISO 9001; REACH (Europe); REACH (UK); RoHS Compliant; SVHC Compliant
- Plastics and Elastomers End Uses
- Profiles
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
- Injection Molding
Technical data
Table 1 of 6
11 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Modulus | 1400.0 | MPa | ISO 178 |
| Flexural Stress (3.5% Strain) | 37.0 | MPa | ISO 178 |
| Tensile Modulus | 1400.0 | MPa | ISO 527 |
| Tensile Stress at Yield | 33.0 | MPa | ISO 527 |
| Tensile Elongation at Yield | 4.0 | % | ISO 527 |
| Tensile Elongation at Break | 15.0 | % | ISO 527 |
| Impact Strength (Charpy, at 23°C) | 220.0 | kJ/m² | ISO 179/1eU |
| Impact Strength (Charpy, at -40°C) | 165.0 | kJ/m² | ISO 179/1eU |
| Notched Impact Strength (Charpy, at 23°C) | 25.0 | kJ/m² | ISO 179/1eA |
| Notched Impact (Charpy, at -40°C) | 7.5 | kJ/m² | ISO 179/1eA |
| Ball Indentation Hardness (H132/30) | 65.0 | MPa | ISO 2039-1 |
Table 2 of 6
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1180.0 | kg/m³ | ISO 1183 |
Table 3 of 6
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Vicat B50 | 85.0 | °C | ISO 306 |
| HDT / A (1.8 MPa) | 82.0 | °C | ISO 75-1/-2 |
Table 4 of 6
1 row| Characteristic | Value | Unit |
|---|---|---|
| Moisture Content | max. 0.05 | % |
Table 5 of 6
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Extrusion Melt Temperature | 180 - 230 | °C |
| Die Temperature | 40 - 80 | °C |
Table 6 of 6
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Index (MVR) | 9.0 | cm³/10min | ISO 1133 |
| MVR Temperature | 210.0 | °C | — |
| MVR Load | 2.16 | kg | — |
| Shrinkage (24h) | 0.8 - 1.1 | % | ISO 294-4 |