To catalogue

Stanyl® TW363

Chemical Family
Polyamides

Stanyl® TW363 is a high-performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear and friction, and process flow qualities are required. This high-performance polyamide 46 is used for applications in automotive, E&E, gears, and outdoor power equipment. Since it retains its mechanical properties at high temperatures up to 220 °C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP. Suitable processing technologies for the product are extrusion and injection molding. Special features include heat stabilization.

Product families

Plastics — Engineering & Specialty Polymers
  • Polyamides

Other characteristics

Brand
Stanyl
Polymer Name
Polyamide 46 (PA 46)
Flexural Modulus
1800.0 - 1800.0 MPa
Additives Included
  • Heat Stabilizer, Lubricant (PTFE)
  • Heat Stabilizer
  • Lubricant (PTFE)
Processing Methods
Extrusion, Injection Molding
Markets
  • Automotive & Transportation
  • Electrical & Electronics
  • Industrial
Technology
Plastics
OEM Standards
  • Callout
  • Chrysler
  • General Motors
  • Volkswagen
  • Volvo
Packaging Type
  • Bags
  • Boxes
  • Silos
  • Super Sacks
Material Features
  • Heat Resistance
  • Heat Stabilized
  • Impact Modified
OEM Specifications
  • CALLOUT ASTM D6779 PA0641Z1
  • CHRYSLER MS-50017 CPN3701
  • GM GMW15702-012271-PA46-I
  • VOLVO STD 121212-1
  • VW 50135 PA46-2-A
Certifications and Compliance
  • ISO 14001
  • OHSAS
  • REACH (Europe)
Plastics and Elastomers End Uses
  • Belt Tensioner
  • Bushings
  • Damping Bands
  • Pump Parts
  • Tubing

Technical data

Table 1 of 7

24 rows
CharacteristicValueUnitMethod
Tensile Modulus1850 / 600MPaISO 527-1/-2
Tensile Modulus (120°C)400 / -MPaISO 527-1/-2
Tensile Modulus (160°C)350 / *MPaISO 527-1/-2
Yield Stress60 / 45MPaISO 527-1/-2
Yield Stress (at 120°C)35 / *MPaISO 527-1/-2
Yield Stress (at 160°C)30 / *MPaISO 527-1/-2
Yield Strain20 / 25%ISO 527-1/-2
Nominal Strain at Break>50 / >50%ISO 527-1/-2
Nominal Strain at Break (at 120°C)>50 / *%ISO 527-1/-2
Nominal Strain at Break (at 160°C)>50 / *%ISO 527-1/-2
Stress at Break (-40°C)85 / -MPaISO 527-1/-2
Strain at Break (at -40°C)66 / -%ISO 527-1/-2

Table 2 of 7

12 rows
CharacteristicValueUnitMethod
Melting Temperature (10°C/min)295 / *°CISO 11357-1/-3
Glass Transition Temperature (at 10°C/min)75 / *°CISO 11357-1/-2
Temperature of Deflection Under Load (1.80 MPa)90 / *°CISO 75-1/-2
Temperature of Deflection Under Load (0.45 MPa)200 / *°CISO 75-1/-2
Vicat Softening Temperature (50°C/h 50N)250 / *°CISO 306
Coefficient of Linear Thermal Expansion (parallel)1.6 / *E-4/°CISO 11359-1/-2
Coefficient of Linear Thermal Expansion (normal)1.8 / *E-4/°CISO 11359-1/-2
Oxygen Index27 / *%ISO 4589-1/-2
Thermal Index (2500 hrs)150 / *°CIEC 60216/ISO 527-1/-2
Thermal Index (5000 hrs)135 / *°CIEC 60216/ISO 527-1/-2
Thermal Index (10000 hrs)120 / *°CIEC 60216/ISO 527-1/-2
Thermal Index (20000 hrs)105 / *°CIEC 60216/ISO 527-1/-2

Table 3 of 7

8 rows
CharacteristicValueUnitMethod
Relative Permittivity (100Hz)3.6 / 14—IEC 62631-2-1
Relative Permittivity (1 MHz)3.2 / 4—IEC 62631-2-1
Dissipation Factor (100 Hz)120 / 6500E-4IEC 62631-2-1
Dissipation Factor (1 MHz)190 / 1000E-4IEC 62631-2-1
Volume Resistivity1E13 / 1E7Ohm*mIEC 62631-3-1
Surface Resistivity- / 1E13OhmIEC 62631-3-2
Electric Strength25 / 15kV/mmIEC 60243-1
Comparative Tracking Index475 / -VIEC 60112

Table 4 of 7

4 rows
CharacteristicValueUnit
Density of Melt913 / *kg/m³
Thermal Conductivity of Melt0.24 / *W/(m K)
Specific Heat Capacity Melt2550 / *J/(kg K)
Effective Thermal Diffusivity9.82E-7 / *m²/s

Table 5 of 7

4 rows
CharacteristicValueUnitMethod
Water Absorption11 / *%Sim. to ISO 62
Water Absorption in Water (at 23°C after 24h)3 / *%ISO 62
Humidity Absorption2.95 / *%Sim. to ISO 62
Density1100 / -kg/m³ISO 1183

Table 6 of 7

2 rows
CharacteristicValueUnitMethod
Molding Shrinkage (parallel)2 / *%Sim. to ISO 294-4
Molding Shrinkage (normal)2 / *%Sim. to ISO 294-4

Химическая стойкость

377 rows
CharacteristicValueUnit
OtherAcetaldehyde (40% by mass) at 23°Cresistant
OtherAcetamide (50% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetamide (50% by mass) at >140°Cnot resistant
OtherAcetic acid (10% by mass) at 100°Cnot resistant
OtherAcetic acid (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetic acid (95% by mass) at 23°Cnot resistant
KetonesAcetone at 23°Cresistant
OtherAcetophenone at 23°Cresistant
OtherAcetyl chloride at 23°Cnot resistant
OtherAcetylene at 23°Cresistant
OtherAcrylic acid at 23°Cnot resistant
OtherAliphatic amines at 23°Cresistant