Akulon® RePurposed RE BK00003
- Chemical Family
- Polyamides
Akulon® RePurposed RE BK00003 is a high-performance material that incorporates both polyamide 6 and polyamide 66. It is a widely utilized material by customers globally, finding applications in various industries, including automotive, electronics, electrical, furniture, and packaging. In molded parts, this material excels in providing an impressive balance between ease of design and processing, all while delivering outstanding mechanical properties across a broad temperature range and under diverse conditions.
Product families
- Polyamides
Other characteristics
- Brand
- Akulon®
- Polymer Name
- Polyamide 6 (PA 6)
- Processing Methods
- Injection Molding
- Markets
- Automotive & Transportation
- Consumer Goods
- Electrical & Electronics
- Technology
- Plastics
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Labeling Claims
- Recycled
- Sustainable
- Material Features
- Dimensional Stability
- Good Strength
- High Durability
- Light Weight
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
- Plastics and Elastomers End Uses
- Door Panel
- Flooring
- Surfboards
- Wheel Housing Parts
- Machinery for Injection Molding
Central bushing heated separately; Only use external heated system; Manifold heated from both sides; Tip with thermocouple in front (near gate); Very accurate temperature control in the gate area
- Plastics and Elastomers Functions
- Resin
- Grade Coding for Injection Molding
Akulon® PA6 non reinforced and non flame retardant injection molding grades.
Technical data
Table 1 of 6
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 3000 / - | MPa | ISO 527-1/-2 |
| Yield Stress | 70 / - | MPa | ISO 527-1/-2 |
| Yield Strain | 3 / - | % | ISO 527-1/-2 |
| Nominal Strain at Break | 14 / - | % | ISO 527-1/-2 |
| Charpy Impact Strength (at +23°C) | N / - | kJ/m² | ISO 179/1eU |
| Charpy Notched Impact Strength (at +23°C) | 6 / - | kJ/m² | ISO 179/1eA |
Table 2 of 6
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature (10°C/min) | 220 / * | °C | ISO 11357-1/-3 |
| Temperature of Deflection Under Load (1.80 MPa) | 60 / * | °C | ISO 75-1/-2 |
| Temperature of Deflection Under Load (0.45 MPa) | 150 / * | °C | ISO 75-1/-2 |
| Ball Pressure Temperature | 180 / * | °C | IEC 60695-10-2 |
| Glow Wire Flammability Index (at thickness 0.75 / - mm) | 725 / - | °C | IEC 60695-2-12 |
| Glow Wire Flammability Index (at thickness 3 / - mm) | 675 / - | °C | IEC 60695-2-12 |
Table 3 of 6
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Comparative Tracking Index | 575 / - | V | IEC 60112 |
Table 4 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water Absorption | 9 / * | % | Sim. to ISO 62 |
| Humidity Absorption | 2.5 / * | % | Sim. to ISO 62 |
| Density | 1140 / - | kg/m³ | ISO 1183 |
Table 5 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Volume-Flow Rate (at 235 / * °C, 5 / * kg) | 90 / * | cm³/10min | ISO 1133 |
| Molding Shrinkage (parallel) | 1.1 / * | % | ISO 294-4 |
| Molding Shrinkage (normal) | 1.1 / * | % | ISO 294-4 |
Химическая стойкость
385 rows| Characteristic | Value | Unit |
|---|---|---|
| Other | Acetaldehyde (40% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at >140°C | not resistant |
| Other | Acetic acid (10% by mass) at 100°C | not resistant |
| Other | Acetic acid (10% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetic acid (95% by mass) at 23°C | not resistant |
| Ketones | Acetone at 23°C | resistant |
| Other | Acetophenone at 23°C | resistant |
| Other | Acetyl chloride at 23°C | not resistant |
| Other | Acetylene at 23°C | resistant |
| Other | Acrylic acid at 23°C | not resistant |
| Other | Aliphatic amines at 23°C | resistant |