Stanyl® TW341-N
- Chemical Family
- Polyamides
Stanyl® TW341-N is a high-performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear and friction, and process flow qualities are required. This high-performance polyamide 46 is used for applications in automotive, E&E, gears, and outdoor power equipment. Since it retains its mechanical properties at high temperatures up to 220 °C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP. A suitable processing technology for the product is injection molding. Special features include being heated, stabilized, and lubricated.
Product families
- Polyamides
Other characteristics
- Brand
- Stanyl
- Polymer Name
- Polyamide 46 (PA 46)
- Flexural Modulus
- 3000.0 - 3000.0 MPa
- Additives Included
Heat Stabilizer, Lubricant (PTFE), Lubricant (Unspecified); Heat Stabilizer; Lubricant (PTFE); Lubricant (Unspecified)
- Processing Methods
- Injection Molding
- Markets
- Automotive & Transportation
- Consumer Goods
- Electrical & Electronics
- Technology
- Plastics
- OEM Standards
- Mercedes
- Volkswagen
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Material Features
- Friction Resistant
- Heat Resistance
- Heat Stabilized
- Lubricated
- Wear Resistant
- OEM Specifications
- MERCEDES DBL 5403.50
- VW 50135 PA46-1A
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
Technical data
Table 1 of 8
28 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 3300 / 1000 | MPa | ISO 527-1/-2 |
| Tensile Modulus (120°C) | 800 / - | MPa | ISO 527-1/-2 |
| Tensile Modulus (160°C) | 650 / * | MPa | ISO 527-1/-2 |
| Tensile Modulus (180°C) | 600 / * | MPa | ISO 527-1/-2 |
| Tensile Modulus (200°C) | 500 / * | MPa | ISO 527-1/-2 |
| Yield Stress | 100 / 55 | MPa | ISO 527-1/-2 |
| Yield Stress (at 120°C) | 50 / * | MPa | ISO 527-1/-2 |
| Yield Stress (at 160°C) | 40 / * | MPa | ISO 527-1/-2 |
| Yield Stress (at 180°C) | 35 / * | MPa | ISO 527-1/-2 |
| Yield Stress (at 200°C) | 30 / * | MPa | ISO 527-1/-2 |
| Yield Strain | 10 / 20 | % | ISO 527-1/-2 |
| Nominal Strain at Break | 40 / >50 | % | ISO 527-1/-2 |
Table 2 of 8
16 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature (10°C/min) | 295 / * | °C | ISO 11357-1/-3 |
| Glass Transition Temperature (at 10°C/min) | 75 / * | °C | ISO 11357-1/-2 |
| Temperature of Deflection Under Load (1.80 MPa) | 190 / * | °C | ISO 75-1/-2 |
| Temperature of Deflection Under Load (0.45 MPa) | 280 / * | °C | ISO 75-1/-2 |
| Vicat Softening Temperature (50°C/h 50N) | 290 / * | °C | ISO 306 |
| Coefficient of Linear Thermal Expansion (parallel) | 0.85 / * | E-4/°C | ISO 11359-1/-2 |
| Coefficient of Linear Thermal Expansion (normal) | 1.1 / * | E-4/°C | ISO 11359-1/-2 |
| Oxygen Index | 27 / * | % | ISO 4589-1/-2 |
| Glow Wire Flammability Index (at thickness 3 / - mm) | 650 / - | °C | IEC 60695-2-12 |
| Glow Wire Flammability Index (at thickness 0.75 / - mm) | 750 / - | °C | IEC 60695-2-12 |
| Glow Wire Ignition Temperature (at thickness 3 / - mm) | 700 / - | °C | IEC 60695-2-13 |
| Glow Wire Ignition Temperature (at thickness 0.75 / - mm) | 725 / - | °C | IEC 60695-2-13 |
Table 3 of 8
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Relative Permittivity (100Hz) | 3.9 / 22 | — | IEC 62631-2-1 |
| Relative Permittivity (1 MHz) | 3.6 / 4.5 | — | IEC 62631-2-1 |
| Dissipation Factor (100 Hz) | 70 / 8700 | E-4 | IEC 62631-2-1 |
| Dissipation Factor (1 MHz) | 260 / 1200 | E-4 | IEC 62631-2-1 |
| Volume Resistivity | 1E13 / 1E7 | Ohm*m | IEC 62631-3-1 |
| Surface Resistivity | - / 1E13 | Ohm | IEC 62631-3-2 |
| Electric Strength | 25 / 15 | kV/mm | IEC 60243-1 |
| Comparative Tracking Index | 400 / - | V | IEC 60112 |
Table 4 of 8
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Viscosity Number | 185 / * | cm³/g | ISO 307, 1157, 1628 |
Table 5 of 8
3 rows| Characteristic | Value | Unit |
|---|---|---|
| Density of Melt | 990 / * | kg/m³ |
| Thermal Conductivity of Melt | 0.25 / * | W/(m K) |
| Specific Heat Capacity Melt | 2670 / * | J/(kg K) |
Table 6 of 8
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water Absorption | 13.5 / * | % | Sim. to ISO 62 |
| Water Absorption in Water (at 23°C after 24h) | 3.8 / * | % | ISO 62 |
| Humidity Absorption | 3.7 / * | % | Sim. to ISO 62 |
| Density | 1180 / - | kg/m³ | ISO 1183 |
Table 7 of 8
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Molding Shrinkage (parallel) | 2 / * | % | Sim. to ISO 294-4 |
| Molding Shrinkage (normal) | 2 / * | % | Sim. to ISO 294-4 |
| Spiral Flow Length 1.0 mm 800 bar | 110 / * | mm | — |
| Spiral Flow Length 1.0 mm 900 bar | 120 / * | mm | — |
| Spiral Flow Length 1.0 mm 1000 bar | 130 / * | mm | — |
| Spiral Flow Length 0.5mm 1200 bar | 60 / * | mm | — |
| Spiral Flow Length 0.5 mm 1600 bar | 70 / * | mm | — |
| Spiral Flow Length 0.5mm 2000 bar | 90 / * | mm | — |
Химическая стойкость
377 rows| Characteristic | Value | Unit |
|---|---|---|
| Other | Acetaldehyde (40% by mass) at 23°C | resistant |
| Other | Acetamide (50% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at >140°C | not resistant |
| Other | Acetic acid (10% by mass) at 100°C | not resistant |
| Other | Acetic acid (10% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetic acid (95% by mass) at 23°C | not resistant |
| Ketones | Acetone at 23°C | resistant |
| Other | Acetophenone at 23°C | resistant |
| Other | Acetyl chloride at 23°C | not resistant |
| Other | Acetylene at 23°C | resistant |
| Other | Acrylic acid at 23°C | not resistant |
| Other | Aliphatic amines at 23°C | resistant |