Stanyl® TC170
- Chemical Family
- Polyamides
Stanyl® TC170 is a high-performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear and friction, and process flow qualities are required. This high-performance polyamide 46 is used for applications in automotive, E&E, gears, and outdoor power equipment. Since it retains its mechanical properties at high temperatures up to 220 °C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP. A suitable processing technology for the product is injection molding. Special features include laser marking and thermal conductivity.
Product families
- Polyamides
Other characteristics
- Brand
- Stanyl
- Polymer Name
- Polyamide (unspecified)
- Fillers Included
- Glass Fiber
- Flexural Modulus
- 12000.0 - 12000.0 MPa
- Processing Methods
- Injection Molding
- Markets
- Consumer Goods
- Applications
- Consumer Goods — Appliances & Electronics
- Technology
- Plastics
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Material Features
- Good Thermal Conductivity
- Heat Resistance
- Laser Markable
- Thermally Conductive
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 6
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 12500 / 7100 | MPa | ISO 527-1/-2 |
| Stress at Break | 130 / 80 | MPa | ISO 527-1/-2 |
| Strain at Break | 2.5 / 5.2 | % | ISO 527-1/-2 |
| Flexural Modulus | 12000 / 7200 | MPa | ISO 178 |
| Flexural Strength | 200 / 135 | MPa | ISO 178 |
| Charpy Impact Strength (at +23°C) | 55 / 60 | kJ/m² | ISO 179/1eU |
| Charpy Notched Impact Strength (at +23°C) | 9 / 13 | kJ/m² | ISO 179/1eA |
Table 2 of 6
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Temperature of Deflection Under Load (1.80 MPa) | 210 / * | °C | ISO 75-1/-2 |
| Coefficient of Linear Thermal Expansion (parallel) | 0.2 / * | E-4/°C | ISO 11359-1/-2 |
| Coefficient of Linear Thermal Expansion (normal) | 0.9 / * | E-4/°C | ISO 11359-1/-2 |
| Thermal Conductivity in Plane | 2.1 / * | W/(m K) | ASTM E1461 |
| Thermal Conductivity Through Plane | 0.9 / * | W/(m K) | ASTM E1461 |
Table 3 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Volume Resistivity | >1E13 / 4E12 | Ohm*m | IEC 62631-3-1 |
| Surface Resistivity | - / 2E11 | Ohm | IEC 62631-3-2 |
| Comparative Tracking Index | 350 / - | V | IEC 60112 |
Table 4 of 6
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Humidity Absorption | 1.6 / * | % | Sim. to ISO 62 |
| Density | 1550 / - | kg/m³ | ISO 1183 |
Table 5 of 6
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Molding Shrinkage (parallel) | 0.25 / * | % | ISO 294-4 |
| Molding Shrinkage (normal) | 0.6 / * | % | ISO 294-4 |
Химическая стойкость
377 rows| Characteristic | Value | Unit |
|---|---|---|
| Other | Acetaldehyde (40% by mass) at 23°C | resistant |
| Other | Acetamide (50% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at >140°C | not resistant |
| Other | Acetic acid (10% by mass) at 100°C | not resistant |
| Other | Acetic acid (10% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetic acid (95% by mass) at 23°C | not resistant |
| Ketones | Acetone at 23°C | resistant |
| Other | Acetophenone at 23°C | resistant |
| Other | Acetyl chloride at 23°C | not resistant |
| Other | Acetylene at 23°C | resistant |
| Other | Acrylic acid at 23°C | not resistant |
| Other | Aliphatic amines at 23°C | resistant |