To catalogue

Akulon® K225-KV

Chemical Family
Polyamides

Akulon® K225-KV is a polyamide 6 (PA 6) resin, an injection-molded polymer with a heat stabilizer that is halogen-free. It features flame-retardant properties, is heat-stable, and has a light weight. Additionally, it is UL flame-rated, making it suitable for applications in the automotive and transportation industries.

Product families

Applications

Automotive & Transportation — Automotive
  • Exterior & Body
  • Interior

Product Families

Plastics — Engineering & Specialty Polymers
  • Polyamides

Other characteristics

Brand
Akulon®
Polymer Name
Polyamide 6 (PA 6)
Additives Included
Heat Stabilizer
Processing Methods
Injection Molding
Markets
Automotive & Transportation
Flame Rating
UL 94 V2
Technology
Plastics
Packaging Type
  • Bags
  • Boxes
  • Silos
  • Super Sacks
Labeling Claims
Halogen-free
Quality Standards
  • UL Yellow Card (E43392)
  • UL Yellow Card (E47960)
Material Features
  • Flame Retardant
  • Heat Stabilized
  • Light Weight
  • UL Flame Rated
Certifications and Compliance
  • ISO 14001
  • OHSAS
  • REACH (Europe)
  • UL 94
Plastics and Elastomers End Uses
  • Door Panel
  • Flooring
  • Wheel Housing Parts
Machinery for Injection Molding

Central bushing heated separately; Only use external heated system; Manifold heated from both sides; Tip with thermocouple in front (near gate); Very accurate temperature control in the gate area

Plastics and Elastomers Functions
Resin

Technical data

Table 1 of 6

7 rows
CharacteristicValueUnitMethod
Tensile Modulus4200 / 1600MPaISO 527-1/-2
Yield Stress70 / 35MPaISO 527-1/-2
Yield Strain3 / 30%ISO 527-1/-2
Nominal Strain at Break4 / >50%ISO 527-1/-2
Charpy Impact Strength (at +23°C)40 / -kJ/m²ISO 179/1eU
Charpy Notched Impact Strength (at +23°C)4 / 9kJ/m²ISO 179/1eA
Charpy Notched Impact Strength (at -30°C)3 / 5kJ/m²ISO 179/1eA

Table 2 of 6

15 rows
CharacteristicValueUnitMethod
Melting Temperature (10°C/min)220 / *°CISO 11357-1/-3
Burning Behaviour (at 1.5 mm Nominal Thickness)UL V-2 / *classIEC 60695-11-10
Burning Behaviour (at 3.0 mm Nominal Thickness)UL V-2 / *classIEC 60695-11-10
Burning Behaviour (at 0.4 mm Nominal Thickness)V-2 / *classIEC 60695-11-10
Burning Behaviour (at 0.75 mm Nominal Thickness)V-2 / *classIEC 60695-11-10
Glow Wire Flammability Index (at thickness 0.38 / - mm)960 / -°CIEC 60695-2-12
Glow Wire Flammability Index (at thickness 3 / - mm)960 / -°CIEC 60695-2-12
Glow Wire Ignition Temperature (at thickness 0.38 / - mm)930 / -°CIEC 60695-2-13
Glow Wire Ignition Temperature (at thickness 3 / - mm)850 / -°CIEC 60695-2-13
Relative Temperature Index (Electrical, 0.38 / * mm)150 / *°CUL746B
Relative Temperature Index (Electrical, 3 / * mm)150 / *°CUL746B
Relative Temperature Index (with impact, 0.38 / * mm)80 / *°CUL746B

Table 3 of 6

8 rows
CharacteristicValueUnitMethod
Relative Permittivity (100Hz)3.3 / 8—IEC 62631-2-1
Relative Permittivity (1 MHz)3.2 / 3.6—IEC 62631-2-1
Dissipation Factor (100 Hz)90 / 1250E-4IEC 62631-2-1
Dissipation Factor (1 MHz)200 / 800E-4IEC 62631-2-1
Volume Resistivity>1E13 / 1E11Ohm*mIEC 62631-3-1
Surface Resistivity- / 1E14OhmIEC 62631-3-2
Electric Strength30 / 25kV/mmIEC 60243-1
Comparative Tracking Index600 / -VIEC 60112

Table 4 of 6

3 rows
CharacteristicValueUnitMethod
Water Absorption7.5 / *%Sim. to ISO 62
Humidity Absorption2 / *%Sim. to ISO 62
Density1210 / -kg/m³ISO 1183

Table 5 of 6

2 rows
CharacteristicValueUnitMethod
Molding Shrinkage (parallel)1 / *%ISO 294-4
Molding Shrinkage (normal)1 / *%ISO 294-4

Химическая стойкость

385 rows
CharacteristicValueUnit
OtherAcetaldehyde (40% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetamide (50% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetamide (50% by mass) at >140°Cnot resistant
OtherAcetic acid (10% by mass) at 100°Cnot resistant
OtherAcetic acid (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetic acid (95% by mass) at 23°Cnot resistant
KetonesAcetone at 23°Cresistant
OtherAcetophenone at 23°Cresistant
OtherAcetyl chloride at 23°Cnot resistant
OtherAcetylene at 23°Cresistant
OtherAcrylic acid at 23°Cnot resistant
OtherAliphatic amines at 23°Cresistant