Arnite® TV4 264 SN
Arnite® TV4 264 SN is a high-performance engineering plastic that offers a combination of high strength, rigidity, and excellent processing characteristics. It is well-suited for a wide range of applications in the automotive, electrical, electronic, and consumer goods industries. The preferred processing technology for Arnite® TV4 264 SN is injection molding, which allows for efficient and precise manufacturing of components.
Product families
Applications
- Switches & Relays
Product Families
- Polyesters & Copolyesters
Other characteristics
- Brand
- Arnite
- Polymer Name
- Polybutylene Terephthalate (PBT)
- Fillers Included
- Glass Fiber
- Processing Methods
- Injection Molding
- Markets
- Electrical & Electronics
- Flame Rating
- UL 94 V0
- Technology
- Plastics
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Quality Standards
- UL Yellow Card (E43392)
- UL Yellow Card (E47960)
- Material Features
- Flame Retardant
- UL Flame Rated
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
- UL 94
- Plastics and Elastomers End Uses
- Relay Bases
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
- Motor Starter/Overload Relays Application Data
Akulon® PA6, Arnite® PBT, Stanyl® PA46 and ForTii® PA4T allow for reliable solutions due to good electrical and thermal endurance. Akulon® PA6, Arnite® PBT, Stanyl® PA46 and ForTii® PA4T allow for more design freedom and/or potential system cost reductions due to part integration and thinner wall design and lower profiles possibilities, reduced cycle time with lower production losses
Technical data
Table 1 of 6
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 11500 | MPa | ISO 527-1/-2 |
| Stress at Break | 140 | MPa | ISO 527-1/-2 |
| Strain at Break | 1.8 | % | ISO 527-1/-2 |
| Charpy Impact Strength (at +23°C) | 45 | kJ/m² | ISO 179/1eU |
| Charpy Impact Strength (at -30°C) | 45 | kJ/m² | ISO 179/1eU |
| Charpy Notched Impact Strength (at +23°C) | 6.3 | kJ/m² | ISO 179/1eA |
| Charpy Notched Impact Strength (at -30°C) | 8 | kJ/m² | ISO 179/1eA |
Table 2 of 6
13 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature (10°C/min) | 225 | °C | ISO 11357-1/-3 |
| Temperature of Deflection Under Load (1.80 MPa) | 210 | °C | ISO 75-1/-2 |
| Temperature of Deflection Under Load (0.45 MPa) | 220 | °C | ISO 75-1/-2 |
| Coefficient of Linear Thermal Expansion (parallel) | 0.35 | E-4/°C | ISO 11359-1/-2 |
| Coefficient of Linear Thermal Expansion (normal) | 0.7 | E-4/°C | ISO 11359-1/-2 |
| Burning Behaviour (at 1.5 mm Nominal Thickness) | UL V-0 | class | IEC 60695-11-10 |
| Burning Behaviour (at 3.0 mm Nominal Thickness) | UL V-0 | class | IEC 60695-11-10 |
| Relative Temperature Index (Electrical, 0.4 mm) | 75 | °C | UL746B |
| Relative Temperature Index (Electrical, 3 mm) | 140 | °C | UL746B |
| Relative Temperature Index (with impact, 0.4 mm) | 75 | °C | UL746B |
| Relative Temperature Index (with impact, 3 mm) | 110 | °C | UL746B |
| Relative Temperature Index (without impact, 0.4 mm) | 75 | °C | UL746B |
Table 3 of 6
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Relative Permittivity (100Hz) | 3.7 | — | IEC 62631-2-1 |
| Relative Permittivity (1 MHz) | 3.5 | — | IEC 62631-2-1 |
| Dissipation Factor (100 Hz) | 20 | E-4 | IEC 62631-2-1 |
| Dissipation Factor (1 MHz) | 160 | E-4 | IEC 62631-2-1 |
| Volume Resistivity | >1E13 | Ohm*m | IEC 62631-3-1 |
| Comparative Tracking Index | 200 | V | IEC 60112 |
Table 4 of 6
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Density of Melt | 1440 | kg/m³ |
| Thermal Conductivity of Melt | 0.153 | W/(m K) |
| Specific Heat Capacity Melt | 1740 | J/(kg K) |
| Effective Thermal Diffusivity | 6.12E-8 | m²/s |
Table 5 of 6
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1700 | kg/m³ | ISO 1183 |
Химическая стойкость
283 rows| Characteristic | Value | Unit |
|---|---|---|
| Other | Acetic acid (10% by mass) at 23°C | not resistant |
| Other | Acetic acid (95% by mass) at 23°C | not resistant |
| Ketones | Acetone at 23°C | limited resistant, tests necessary to verify |
| Other | Acetophenone at 23°C | resistant |
| Other | Acetylene at 23°C | resistant |
| Other | Aliphatic amines at 23°C | resistant |
| Other | Aliphatic hydrocarbons at 23°C | resistant |
| Other | Allyl alcohol at 23°C | resistant |
| Other | Aluminum acetate (saturated) at 23°C | resistant |
| Other | Aluminum hydroxide (saturated) at 23°C | resistant |
| Other | Aluminum salts of mineral acids (saturated) at 23°C | resistant |
| Other | Amino acids (saturated) at 23°C | resistant |