Akulon® K224-G6-FC NA99001
- Chemical Family
- Polyamides
Akulon® K224-G6-FC NA99001 is a polyamide 6 (PA 6) resin labeled as food contact acceptable. This product possesses features like being lightweight and UL flame-rated. This is used in markets associated with automotive and transportation, as well as healthcare and pharma. End uses of this product are in door panels, flooring, and wheel housing parts.
Other characteristics
- Brand
- Akulon®
- Polymer Name
- Polyamide 6 (PA 6)
- Fillers Included
- Glass Fiber
- Processing Methods
- Injection Molding, Injection Molding
- Reinforcement Material
- Glass Fibers
- Safety
For the safety properties of the material, we refer to our SDS which can be ordered at our sales offices. During practical operation we advise to wear personal safety protections for hand/eye/body.
- Markets
- Automotive & Transportation
- Healthcare & Pharma
- PACKAGING
Akulon® grades are supplied in airtight, moisture- proof packaging.
- Flame Rating
- UL 94 HB
- Technology
- Composite Materials
- Plastics
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Labeling Claims
- Food Contact Acceptable
- Quality Standards
- UL Yellow Card (E47960)
- Material Features
- Food Contact Acceptable
- Light Weight
- UL Flame Rated
- Reinforcement Form
- Tape
- Unidirectional Fabric
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
- UL 94
- Composite Materials Functions
- Resins Binders & Matrix Materials
- Composites Processing Methods
- Injection Molding
- Plastics and Elastomers End Uses
- Door Panel
- Flooring
- Wheel Housing Parts
- Plastics and Elastomers Functions
- Resin
Technical data
Table 1 of 8
9 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 9500 / 6000 | MPa | ISO 527-1/-2 |
| Stress at Break | 180 / 110 | MPa | ISO 527-1/-2 |
| Strain at Break | 3.5 / 7 | % | ISO 527-1/-2 |
| Flexural Modulus | 8600 / - | MPa | ISO 178 |
| Flexural Strength | 235 / - | MPa | ISO 178 |
| Charpy Impact Strength (at +23°C) | 90 / 110 | kJ/m² | ISO 179/1eU |
| Charpy Impact Strength (at -30°C) | 75 / 75 | kJ/m² | ISO 179/1eU |
| Charpy Notched Impact Strength (at +23°C) | 12 / 25 | kJ/m² | ISO 179/1eA |
| Charpy Notched Impact Strength (at -30°C) | 11 / 11 | kJ/m² | ISO 179/1eA |
Table 2 of 8
14 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature (10°C/min) | 220 / * | °C | ISO 11357-1/-3 |
| Temperature of Deflection Under Load (1.80 MPa) | 200 / * | °C | ISO 75-1/-2 |
| Temperature of Deflection Under Load (0.45 MPa) | 220 / * | °C | ISO 75-1/-2 |
| Coefficient of Linear Thermal Expansion (parallel) | 0.2 / * | E-4/°C | ISO 11359-1/-2 |
| Coefficient of Linear Thermal Expansion (normal) | 0.7 / * | E-4/°C | ISO 11359-1/-2 |
| Burning Behaviour (at 1.5 mm Nominal Thickness) | UL HB / * | class | IEC 60695-11-10 |
| Burning Behaviour (at 3.0 mm Nominal Thickness) | UL HB / * | class | IEC 60695-11-10 |
| Burning Behaviour (at 0.75 mm Nominal Thickness) | HB / * | class | IEC 60695-11-10 |
| Relative Temperature Index (Electrical, 0.75 / * mm) | 65 / * | °C | UL746B |
| Relative Temperature Index (Electrical, 3 / * mm) | 65 / * | °C | UL746B |
| Relative Temperature Index (with impact, 0.75 / * mm) | 65 / * | °C | UL746B |
| Relative Temperature Index (with impact, 3 / * mm) | 65 / * | °C | UL746B |
Table 3 of 8
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Relative Permittivity (100Hz) | 3.5 / 20 | — | IEC 62631-2-1 |
| Relative Permittivity (1 MHz) | 3.3 / 5 | — | IEC 62631-2-1 |
| Dissipation Factor (100 Hz) | 50 / 3000 | E-4 | IEC 62631-2-1 |
| Dissipation Factor (1 MHz) | 150 / 1200 | E-4 | IEC 62631-2-1 |
| Volume Resistivity | 1E13 / 1E11 | Ohm*m | IEC 62631-3-1 |
| Surface Resistivity | - / 1E14 | Ohm | IEC 62631-3-2 |
| Electric Strength | 30 / 25 | kV/mm | IEC 60243-1 |
| Comparative Tracking Index | - / 600 | V | IEC 60112 |
Table 4 of 8
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Density of Melt | 1150 / * | kg/m³ |
| Thermal Conductivity of Melt | 0.27 / * | W/(m K) |
| Specific Heat Capacity Melt | 2110 / * | J/(kg K) |
| Effective Thermal Diffusivity | 1.12E-7 / * | m²/s |
Table 5 of 8
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water Absorption | 6.3 / * | % | Sim. to ISO 62 |
| Humidity Absorption | 1.9 / * | % | Sim. to ISO 62 |
| Density | 1350 / - | kg/m³ | ISO 1183 |
Table 6 of 8
1 row| Characteristic | Value | Method |
|---|---|---|
| Shore D Hardness (15s) | 85 / * | ISO 868 |
Table 7 of 8
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Volume-Flow Rate (at 240 / * °C, 2.16 / * kg) | 6.4 / * | cm³/10min | ISO 1133 |
| Melt Flow Index (at 240 / * °C, 2.16 / * kg) | 7.3 / * | g/10min | ISO 1133 |
| Molding Shrinkage (parallel) | 0.3 / * | % | ISO 294-4 |
| Molding Shrinkage (normal) | 0.9 / * | % | ISO 294-4 |
Химическая стойкость
385 rows| Characteristic | Value | Unit |
|---|---|---|
| Other | Acetaldehyde (40% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at >140°C | not resistant |
| Other | Acetic acid (10% by mass) at 100°C | not resistant |
| Other | Acetic acid (10% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetic acid (95% by mass) at 23°C | not resistant |
| Ketones | Acetone at 23°C | resistant |
| Other | Acetophenone at 23°C | resistant |
| Other | Acetyl chloride at 23°C | not resistant |
| Other | Acetylene at 23°C | resistant |
| Other | Acrylic acid at 23°C | not resistant |
| Other | Aliphatic amines at 23°C | resistant |