Arnitel® UM551-V is a high-performance thermoplastic copolyester (TPC) known for its combination of flexibility, high temperature resistance, and strength, complemented by excellent processing characteristics. In industries such as automotive and E&E, Arnitel® UM551-V is becoming a more sustainable and efficient alternative to traditional rubbers, leading to reduced environmental impact and lower system costs. It's important to note that this material is flame retardant (halogen-phosphorus-free) and should be used in dry environments due to limited hydrolysis resistance. Arnitel® UM551-V can be processed using both extrusion and injection molding technologies, offering versatility for various applications.
Product families
Applications
- Consumer Goods — Furniture
- Cooling & Climate
- Electrical & Electronic Systems
- Equipment & Parts
- Automotive Electronics
- Jacketing & Insulation
Product Families
- Thermoplastic Polyester Elastomers (TPE-E)
Other characteristics
- Brand
- Arnitel
- Density
- 1280.0 - 1280.0 kg/m³
- End Uses
- Pump Parts
- Polymer Name
- Thermoplastic Copolyester Elastomer (TPC-ET)
- Strain at Break
- 50.0 - 50.0 %
- Processing Methods
- Extrusion, Injection Molding
- Markets
- Automotive & Transportation
- Consumer Goods
- Electrical & Electronics
- Industrial
- Flame Rating
- UL 94 V2
- Technology
- Elastomers
- OEM Standards
- Ford
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Labeling Claims
- Halogen-free
- Phosphorus-free
- Quality Standards
- UL Yellow Card (E47960)
- Material Features
- Flame Retardant
- UL Flame Rated
- OEM Specifications
- FORD WSK-M4D692-A3
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
- UL 94
- Plastics and Elastomers End Uses
- Pump Parts
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
- Injection Molding
Technical data
Table 1 of 7
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Yield Stress | 15 | MPa | ISO 527-1/-2 |
| Yield Strain | 22 | % | ISO 527-1/-2 |
| Nominal Strain at Break | >50 | % | ISO 527-1/-2 |
| Charpy Notched Impact Strength (at +23°C) | N | kJ/m² | ISO 179/1eA |
| Izod Notched Impact Strength (at +23°C) | N | kJ/m² | ISO 180/1A |
Table 2 of 7
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature (10°C/min) | 200 | °C | ISO 11357-1/-3 |
| Temperature of Deflection Under Load (0.45 MPa) | 85 | °C | ISO 75-1/-2 |
| Vicat Softening Temperature (50°C/h 50N) | 90 | °C | ISO 306 |
| Burning Behaviour (at 1.5 mm Nominal Thickness) | UL V-2 | class | IEC 60695-11-10 |
| Relative Temperature Index (Electrical, 1.5 mm) | 50 | °C | UL746B |
| Relative Temperature Index (with impact, 1.5 mm) | 50 | °C | UL746B |
| Relative Temperature Index (without impact, 1.5 mm) | 50 | °C | UL746B |
Table 3 of 7
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Relative Permittivity (100Hz) | 5.2 | — | IEC 62631-2-1 |
| Dissipation Factor (100 Hz) | 0.02 | E-4 | IEC 62631-2-1 |
| Volume Resistivity | >1E13 | Ohm*m | IEC 62631-3-1 |
| Electric Strength | 20 | kV/mm | IEC 60243-1 |
| Comparative Tracking Index | 600 | V | IEC 60112 |
Table 4 of 7
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water Absorption | 0.6 | % | Sim. to ISO 62 |
| Humidity Absorption | 0.25 | % | Sim. to ISO 62 |
| Density | 1280 | kg/m³ | ISO 1183 |
Table 5 of 7
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 250 | MPa | ISO 527-1/-2 |
| Stress at 10% strain | 13 | MPa | ISO 527-1/-2 |
| Stress at 100% strain | 17.5 | MPa | ISO 527-1/-2 |
| Stress at Break | 27 | MPa | ISO 527-1/-2 |
| Nominal Strain at Break | 375 | % | ISO 527-1/-2 |
| Shore D Hardness (3s) | 55 | — | ISO 868 |
| Shore D Hardness (15s) | 55 | — | ISO 868 |
Table 6 of 7
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Volume-Flow Rate (at 230 / * °C, 2.16 / * kg) | 15 | cm³/10min | ISO 1133 |
| Melt Flow Index (at 230 °C, 2.16 kg) | 14.4 | g/10min | ISO 1133 |
| Molding Shrinkage (parallel) | 1.35 | % | Sim. to ISO 294-4 |
| Molding Shrinkage (normal) | 1.35 | % | Sim. to ISO 294-4 |
Химическая стойкость
24 rows| Characteristic | Value | Unit |
|---|---|---|
| Other | Acetic acid (10% by mass) at 23°C | resistant |
| Ketones | Acetone at 23°C | resistant |
| Other | Ammonium hydroxide (10% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | ASTM 1 at 23°C | resistant |
| Other | ASTM 3 at 23°C | resistant |
| Other | Brake fluids (DOT 3/4) at 23°C | not resistant |
| Other | Calcium chloride (10% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Chloroform at 23°C | not resistant |
| Ethers | Diethyl ether at 23°C | limited resistant, tests necessary to verify |
| Alcohols | Ethanol at 23°C | limited resistant, tests necessary to verify |
| Other | Ethyl Acetate at 23°C | limited resistant, tests necessary to verify |
| Other | Fuel; Diesel at 85°C | resistant |