To catalogue
Arnitel® CM550-S
- Chemical Family
- Polyesters
Arnitel® CM550-S, a high-performance ThermoPlastic Copolyester (TPC) distinguished by its exceptional blend of flexibility, high-temperature resistance, strength, and outstanding processing capabilities. In applications across automotive and E&E industries, it serves as a lighter, more intelligent, and environmentally friendly alternative to traditional rubber. Produced through extrusion technology, it boasts a hardness of 57 Shore D and is flame-retardant.
Product families
Applications
Automotive & Transportation — Automotive
- Electrical & Electronic Systems
Electrical & Electronics — Devices & Assemblies
- Automotive Electronics
Electrical & Electronics — Wire & Cable
- Jacketing & Insulation
Product Families
Elastomers — Thermoplastic Elastomers
- Thermoplastic Polyester Elastomers (TPE-E)
Other characteristics
- Brand
- Arnitel
- Density
- 1310.0 - 1310.0 kg/m³
- End Uses
- Cables, Wires
- Polymer Name
- Thermoplastic Copolyester Elastomer (TPC-ET)
- Strain at Break
- 50.0 - 50.0 %, 590.0 - 590.0 %
- Processing Methods
- Extrusion
- Markets
- Automotive & Transportation
- Electrical & Electronics
- Technology
- Elastomers
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Material Features
- Flame Retardant
- Chemical Resistance
- Limited resistant, tests necessary to verify
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
- Plastics and Elastomers End Uses
- Cables
- Wires
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
Technical data
Table 1 of 7
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Charpy Impact Strength (at 23°C) | N | kJ/m² | ISO 179/1eU |
| Charpy Impact Strength (at -30°C) | N | kJ/m² | ISO 179/1eU |
| Charpy Notched Impact Strength (at -30°C) | 5 | kJ/m² | ISO 179/1eA |
| Charpy Notched Impact Strength (at 23°C) | N | kJ/m² | ISO 179/1eA |
| Izod Notched Impact Strength (-20°C) | N | kJ/m² | ISO 180/1A |
| Izod Notched Impact Strength (-30°C) | 5.4 | kJ/m² | ISO 180/1A |
Table 2 of 7
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature (at 10°C/min) | 205 | °C | ISO 11357-1/-3 |
| Vicat Softening Temperature (at 50°C/h 50N) | 71 | °C | ISO 306 |
Table 3 of 7
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Relative Permittivity (100Hz) | 4.2 | — | IEC 62631-2-1 |
| Relative Permittivity (1 MHz) | 3.5 | — | IEC 62631-2-1 |
| Dissipation Factor (100 Hz) | 180 | E-4 | IEC 62631-2-1 |
| Dissipation Factor (1 MHz) | 495 | E-4 | IEC 62631-2-1 |
| Volume Resistivity | min. 1E13 | Ohm*m | IEC 62631-3-1 |
Table 4 of 7
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Humidity Absorption | 0.11 | % | Sim. to ISO 62 |
| Density | 1310 | kg/m³ | ISO 1183 |
| Water Absorption in Water (at 23°C, after 24h) | 0.26 | % | ISO 62 |
Table 5 of 7
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Stress (at Break, Normal) | 31 | MPa | ISO 527-1/-2 |
| Stress (at 5% Strain, Normal) | 9.6 | MPa | ISO 527-1/-2 |
| Stress (at 10% Strain, Normal) | 13 | MPa | ISO 527-1/-2 |
| Stress (at 50% Strain, Normal) | 16 | MPa | ISO 527-1/-2 |
| Stress (at 100% Strain, Normal) | 15 | MPa | ISO 527-1/-2 |
| Tear Strength (Normal) | 145 | kN/m | ISO 34-1; Method B |
| Tear Strength (Parallel) | 160 | kN/m | ISO 34-1; Method B |
| Strain (at Break, Normal) | 590 | % | ISO 527-1/-2 |
Table 6 of 7
11 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 200 | MPa | ISO 527-1/-2 |
| Compression Set Under Constant Strain (at 70°C) | 52 | % | ISO 815 |
| Stress (at 5% Strain) | 10 | MPa | ISO 527-1/-2 |
| Stress (at 10% Strain) | 14 | MPa | ISO 527-1/-2 |
| Stress (at 50% Strain) | 18 | MPa | ISO 527-1/-2 |
| Stress (at 100% Strain) | 17 | MPa | ISO 527-1/-2 |
| Stress (at Break) | 28 | MPa | ISO 527-1/-2 |
| Strain (at Break) | min. 300 | % | ISO 527-1/-2 |
| Nominal Strain (at Break) | 400 | % | ISO 527-1/-2 |
| Hardness (3s) | 57 | Shore D | ISO 868 |
| Hardness (15s) | 57 | Shore D | ISO 868 |
Table 7 of 7
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Volume Flow Rate (at 230°C, 2.16 kg) | 17 | cm³/10min | ISO 1133 |