To catalogue
Akulon® K222-KMV5/A
- Chemical Family
- Polyamides
Akulon® K222-KMV5/A is a polyamide 6 (PA 6) resin labeled as halogen-free and known for its flame retardant properties, excellent color stability, and lightweight characteristics. They are frequently utilized in the automotive and transportation sectors, particularly in applications related to automotive exteriors, bodies, and interiors.
Product families
Automotive & Transportation — Automotive
- Exterior & Body
- Interior
Other characteristics
- Brand
- Akulon®
- Polymer Name
- Polyamide 6 (PA 6)
- Fillers Included
- Mineral
- Processing Methods
- Injection Molding, Injection Molding
- Reinforcement Material
- Mineral
- Markets
- Automotive & Transportation
- Technology
- Composite Materials
- Plastics
- Packaging Type
- Bags
- Boxes
- Silos
- Super Sacks
- Labeling Claims
- Halogen-free
- Material Features
- Flame Retardant
- Good Color Stability
- Light Weight
- Reinforcement Form
- Tape
- Unidirectional Fabric
- Certifications and Compliance
- ISO 14001
- OHSAS
- REACH (Europe)
- Composite Materials Functions
- Resins Binders & Matrix Materials
- Composites Processing Methods
- Injection Molding
- Plastics and Elastomers End Uses
- Door Panel
- Flooring
- Wheel Housing Parts
- Plastics and Elastomers Functions
- Resin
Technical data
Table 1 of 7
9 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 6500 / 2700 | MPa | ISO 527-1/-2 |
| Stress at Break | 70 / 38 | MPa | ISO 527-1/-2 |
| Strain at Break | 2.5 / 30 | % | ISO 527-1/-2 |
| Flexural Modulus | 6700 / 2700 | MPa | ISO 178 |
| Flexural Strength | 110 / 55 | MPa | ISO 178 |
| Charpy Impact Strength (at +23°C) | 29 / 100 | kJ/m² | ISO 179/1eU |
| Charpy Impact Strength (at -30°C) | 35 / 35 | kJ/m² | ISO 179/1eU |
| Charpy Notched Impact Strength (at +23°C) | 2 / 4 | kJ/m² | ISO 179/1eA |
| Charpy Notched Impact Strength (at -30°C) | 2 / 2 | kJ/m² | ISO 179/1eA |
Table 2 of 7
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature (10°C/min) | 220 / * | °C | ISO 11357-1/-3 |
| Temperature of Deflection Under Load (1.80 MPa) | 110 / * | °C | ISO 75-1/-2 |
| Temperature of Deflection Under Load (0.45 MPa) | 205 / * | °C | ISO 75-1/-2 |
| Coefficient of Linear Thermal Expansion (parallel) | 0.5 / * | E-4/°C | ISO 11359-1/-2 |
| Coefficient of Linear Thermal Expansion (normal) | 0.5 / * | E-4/°C | ISO 11359-1/-2 |
| Glow Wire Flammability Index (at thickness 0.75 / - mm) | 960 / - | °C | IEC 60695-2-12 |
| Glow Wire Flammability Index (at thickness 3 / - mm) | 960 / - | °C | IEC 60695-2-12 |
Table 3 of 7
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Volume Resistivity | >1E13 / - | Ohm*m | IEC 62631-3-1 |
| Surface Resistivity | - / >1E15 | Ohm | IEC 62631-3-2 |
| Comparative Tracking Index | - / 600 | V | IEC 60112 |
Table 4 of 7
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Density of Melt | 1170 / * | kg/m³ |
| Thermal Conductivity of Melt | 0.201 / * | W/(m K) |
| Specific Heat Capacity Melt | 2250 / * | J/(kg K) |
| Effective Thermal Diffusivity | 7.63E-8 / * | m²/s |
Table 5 of 7
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water Absorption | 6.2 / * | % | Sim. to ISO 62 |
| Humidity Absorption | 1.8 / * | % | Sim. to ISO 62 |
| Density | 1380 / - | kg/m³ | ISO 1183 |
Table 6 of 7
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Volume-Flow Rate (at 250 / * °C, 2.16 / * kg) | 20 / * | cm³/10min | ISO 1133 |
| Molding Shrinkage (parallel) | 0.91 / * | % | ISO 294-4 |
| Molding Shrinkage (normal) | 0.82 / * | % | ISO 294-4 |
Химическая стойкость
385 rows| Characteristic | Value | Unit |
|---|---|---|
| Other | Acetaldehyde (40% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetamide (50% by mass) at >140°C | not resistant |
| Other | Acetic acid (10% by mass) at 100°C | not resistant |
| Other | Acetic acid (10% by mass) at 23°C | limited resistant, tests necessary to verify |
| Other | Acetic acid (95% by mass) at 23°C | not resistant |
| Ketones | Acetone at 23°C | resistant |
| Other | Acetophenone at 23°C | resistant |
| Other | Acetyl chloride at 23°C | not resistant |
| Other | Acetylene at 23°C | resistant |
| Other | Acrylic acid at 23°C | not resistant |
| Other | Aliphatic amines at 23°C | resistant |