GEHR POM® C
GEHR POM® C is produced from the continuous operating temperature of this engineering plastic ranges between -40 °C and +100 °C. Based on its toughness combined with high dimensional stability, there is no tendency to stress cracking. The copolymer has high thermal stability and chemical resistance. In particular, the increased hydrolytic stability and resistance to contact with many solvents must be taken into account. This material is frequently found in applications in the food industry, as cleaning processes require resistance to the use of hot water or various chemical agents. Our round rods and sheets in natural or black color comply with the food contact regulations according to 10/2011/EC.
Properties
- Physical Form
- Bars, Custom, Rods, Sheets
- Bars
- Custom
- Rods
- Sheets
Other characteristics
- Brand
- GEHR POM
- Color
- Black, Natural
- Black
- Natural
- Density
- 1390.0 - 1390.0 kg/m³
- Features
Chemical Resistant, Dimensional Stability, Electrically Insulating, Excellent Toughness, Good Environmental Stress Crack Resistance (ESCR), Good Sliding Properties, Good Solvent Resistance, Good Thermal Stability, High Hydrolytic Stability, High Rigidity, High Stiffness, High Strength, Low Water Absorption
- Polymer Name
- Polyacetal Copolymer (POM)
- Odor
- Odorless
- Markets
- Automotive & Transportation
- Building & Construction
- Electrical & Electronics
- Food & Nutrition
- Healthcare & Pharma
- Industrial
- Storage
The products shall be stored indoor to keep away from any source of degradation such as sunlight, UV-jets, ionizing radiation, chemicals.
- Machining
The product can be machined with standard machinery and tools. Before machining the product should be stored at room temperature 24 h. Evacuate swarf to prevent slipping or tripping. Observe the maximum allowable concentration of dust and formaldehyd levels on the working area which apply in your country. Wear safety goggles during machining. General dust limit value: Respirable dust (6 mg/m3); Inhalable dust (10 mg/m3 ).
- Properties
- Pressure tested quality
- High strength and stiffness
- High rigidity (to -40 °C)
- High thermal stability
- Low water absorption
- High dimension stability
- Good electrical insulating properties
- Very good sliding properties
- Flame Rating
- UL 94 HB
- Insoluble In
- Water
- Technology
- Plastics
- Safety Measures
The general industrial safety measures should be considered. A thermal damage during machining should be avoided.
- Product Families
- Plastics — Parts, Shapes & Films
- Form and Condition
- Rods. Sheets. Hollow Rods / Solid
- Material Features
Chemical Resistant; Dimensional Stability; Electrically Insulating; Excellent Toughness; Good Environmental Stress Crack Resistance (ESCR); Good Sliding Properties; Good Solvent Resistance; Good Thermal Stability; High Hydrolytic Stability; High Rigidity; High Stiffness; High Strength; Low Water Absorption
Technical data
Table 1 of 6
9 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength at Yield | 67 | MPa | ISO 527 |
| Elongation at Yield (S) | 22 | % | ISO 527 |
| Tensile Strength at Break | 65 | MPa | ISO 527 |
| Elongation at Break (R) | 28 | % | ISO 527 |
| Impact Strength (an) | No break | kJ/m2 | ISO 179 |
| Notch impact Strength (ak) | 6 | kJ/m2 | ISO 179 |
| Ball Indentation (Rockwell Hardness) | 125 | MPa | ISO 2039 |
| Hardness | 83 | Shore D | ISO 868 |
| Modulus of elasticity (Et) | 2855 | MPa | ISO 527 |
Table 2 of 6
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Specific Gravity | 1.39 | — | ISO 1183 |
| Water Absorption | 0.8 | % | ISO 62 |
| Humidity Absorption | 0.2 | % | ISO 62 |
| Maximum Permissible Service Temperature | 100 | °C | UL746B |
| Lower Permissible Service Temperature | -40 | °C | UL746B |
Table 3 of 6
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Vicat Softening Point (VST/B/50) | 150 | °C | ISO 306 |
| Heat Deflection Temperature (HDT/B) | 155 | °C | ISO 75 |
| Heat Deflection Temperature (HDT/A) | 95 | °C | ISO 75 |
| Coefficient of Linear Thermal Expansion | 1.2 | K-1.10-4 | ISO 11359 |
| Glass Transition Temperature (Tg) | -65 | °C | ISO 3146 |
| Melting Temperature (Tm) | 166 | °C | ISO 3146 |
Table 4 of 6
4 rows| Characteristic | Value | Unit |
|---|---|---|
| Density | 1.39 | g/cm³ |
| Melting Temperature | 160 - 175 | °C |
| Thermal Decomposition | min. 240 | °C |
| Ignition Temperature | 320 - 340 | °C |
Table 5 of 6
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Volume Resistivity | min. 10^13 | Ω.cm | IEC 60093 |
| Surface Resistivity (Ro) | min. 10^13 | Ω | IEC 60093 |
| Dielectric Constant (1MHz) | 38 | — | IEC 60250 |
| Dielectric Loss Factor (1 MHz) | 5 | — | IEC 60250 |
| Dielectric Strength | 40 | kV/mm | IEC 60243-1 |
| Tracking Resistance | CTI 600 | V | IEC 60112 |
Table 6 of 6
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Physiological Indifference (EEC) | Yes | — | — |
| Physiological Indifference (FDA) | Yes | — | — |
| Flammability | HB | — | UL 94 |
| Limiting Oxygen Index (LOI, 9) | 18 | % | ASTM D2863 |