SuperOhm® 3712
- Chemical Family
- Ethylene-Propylene Copolymers (EPR)
Reddish - orange colored polymeric composition in pellet form, based on EPDM rubber containing peroxide curing agent, ready for extrusion in a conventional CV or dry cure extrusion line.
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
- Exploration & Upstream
- Electrical Protection
- Power & Utilities
- Jacketing & Insulation
- Power Transmission & Distribution
Product Families
- EP Rubbers (EPDM)
Other characteristics
- Brand
- SuperOhm
- Density
- 1330.0 - 1370.0 kg/m³
- Polymer Name
- Ethylene Propylene Copolymer
- Processing Methods
- Extrusion
- Color
- Orange
- Red
- Markets
- Electrical & Electronics
- Industrial
- Storage
SUPEROHM® 3728-5 containers should be stored at temperatures below 50°C (120°F) in a dry area to avoid massing of pellets. Product is recommended to be used within 12 months.
- Handling
To ensure health and safety, Material Safety Data Sheets (MSDS) are available and should be consulted prior to use.
- PACKAGING
- 1,750 pounds (794 Kg) per box.
- Cure
- Air Dry
- Chemical Cure
- Technology
- Elastomers
- Certification
Certified Test Results including physical test data are included with each shipment.
- Packaging Type
- Boxes
- Specifications
When extruded and cured consistent with standard safe wire and cable industry practices, cable insulated with SUPEROHM® 3728-5 EPDM insulation will meet or exceed the requirements as specified in the following standards: ASTM D-2802 and D-2770 ICEA S-68-516 NEMA Pub. No. WC-70, WC-71, WC-74 AEIC CS8-00 ANSI / ICEA S-94-649-2000 Class I, II, III IEC Publication 60502 UL 1072 for type MV-90, MV-105
- Labeling Claims
- Halogen-free
- Quality Standards
- ISO 6722 Class A
- SAE J1128
- Material Features
- Cost Effective
- Crosslinkable
- Excellent Flexibility
- Good Colorability
- Good Electrical Properties
- Good Mechanical Properties
- High Performance
- Chemical Inventories
- TSCA (USA)
- Plastics and Elastomers End Uses
- Cables
- Industrial Cable Insulation
- Industrial Cable Jacketing
- Medium Voltage Insulation
- Wires
- Plastics and Elastomers Processing Methods
- Extrusion
Technical data
Table 1 of 3
3 rows| Characteristic | Value | Unit |
|---|---|---|
| Elongation | 210 | % |
| Specific Gravity | 1.33 - 1.37 | — |
| Tensile Strength | 1600 | psi |
Table 2 of 3
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Retained Elongation (7 Days in 121°C Air Oven) | 95 | % |
| Retained Tensile (7 Days in 121°C Air Oven) | 110 | % |
Table 3 of 3
2 rows| Characteristic | Value | Unit |
|---|---|---|
| Dielectric Strength | 800 | V/mil |
| I.R. Constant (at 15.6ºC) | 80000 | MΩ-1000ft |