To catalogue

Ecomass® Compound 1080BI64

Chemical Family
Polyamides

Ecomass® compound 1080BI64 is a barium sulfate-filled polyamide alloy that is recommended to be used in weighting, balancing and radiation shielding applications. This injection molding grade is known for its excellent toughness, and rigidity. Additionally, it is a nontoxic lead substitute thermoplastic.

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Healthcare & Pharma — Medical
  • Medical Devices & Assemblies
Electrical & Electronics — Parts & Components
  • Housings & Enclosures

Product Families

Plastics — Engineering & Specialty Polymers
  • Blends & Alloys
Composite Materials — Polymers & Resins
  • Thermoplastic Resins

Other characteristics

Brand
Ecomass
Density
2000.0 - 2000.0 kg/m³
Polymer Name
Polyamide (unspecified)
Fillers Included
Barium Sulfate
Processing Methods
Injection Molding, Injection Molding
Color
Grey
Markets
  • Electrical & Electronics
  • Healthcare & Pharma
Technology
  • Composite Materials
  • Plastics
Labeling Claims
Non-Toxic
Material Features
  • Ambient Operating Temperature
  • Excellent Toughness
  • Good Rigidity
  • Lead Substitute
  • Non-Toxic
  • Vibration Damping
Certifications and Compliance
RoHS Compliant
Composites Processing Methods
Injection Molding
Plastics and Elastomers End Uses
Radiation Shielding
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 4

1 row
CharacteristicValueMethod
Specific Gravity2.0ASTM D792

Table 2 of 4

6 rows
CharacteristicValueUnitMethod
Tensile Strength6000.0psiASTM D638
Tensile Modulus650000.0psiASTM D638
Tensile Elongation (at break)4.0 - 5.0%ASTM D638
Flexural Modulus550000.0psiASTM D790
Flexural Strength9000.0psiASTM D790
Izod Impact Strength (Notched)2.1ft-lb/inASTM D256

Table 3 of 4

2 rows
CharacteristicValueUnitMethod
Heat Deflection Temperature (at 66 psi)250.0°FASTM D648
Heat Deflection Temperature (at 264 psi)225.0°FASTM D648

Table 4 of 4

4 rows
CharacteristicValueUnitMethod
Melt Temperature Range400 - 490°F—
Mold Temperature Range135 - 180°F—
Mold Shrinkage Rate0.007 - 0.008in/inASTM D955
Pre-Drying Conditions (at 165°F)4.0hours—

The Omnichem website uses cookies. By continuing to use the site, you consent to their use in accordance with our Privacy Policy and to the collection of analytics.