To catalogue

Ecomass® Compound 4703ZC76

Ecomass® compound 4703ZC76 is a stainless steel-filled thermoplastic polyurethane compound that is recommended to be used in weighting, balancing and vibration dampening applications. This injection molding grade is known for its good toughness and flexibility. Additionally, it functions as a nontoxic thermoplastic lead substitute.

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Consumer Goods — Sports & Recreation
Healthcare & Pharma — Medical
  • Medical Devices & Assemblies
Electrical & Electronics — Parts & Components
  • Housings & Enclosures

Product Families

Composite Materials — Polymers & Resins
  • Thermoplastic Resins
Elastomers — Thermoplastic Elastomers
  • Thermoplastic Urethanes (TPU)

Other characteristics

Brand
Ecomass
Density
3400.0 - 3400.0 kg/m³
Polymer Name
Thermoplastic Polyurethane (unspecified)
Fillers Included
Stainless Steel Powder
Processing Methods
Injection Molding, Injection Molding
Color
  • Grey
  • Opaque
Markets
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Technology
  • Composite Materials
  • Elastomers
Labeling Claims
Non-Toxic
Material Features
  • Ambient Operating Temperature
  • Flexible
  • Good Toughness
  • Lead Substitute
  • Low Odor
  • Non-Toxic
  • Vibration Damping
Chemical Inventories
  • AICS (Australia)
  • DSL (Canada)
  • EINECS (EU)
  • ENCS (Japan)
  • IECSC (China)
  • ISHL (Japan)
  • KECI (Korea)
  • PICCS (Phillipines)
Certifications and Compliance
RoHS Compliant
Composites Processing Methods
Injection Molding
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 4

1 row
CharacteristicValueUnitMethod
Density3.4g/ccASTM D792

Table 2 of 4

5 rows
CharacteristicValueUnitMethod
Tensile Elongation at Break200%ASTM D638
Tensile Strength19MPaASTM D638
Tensile Modulus517MPaASTM D638
Flexural Modulus167MPaASTM D790
Flexural Strength41MPaASTM D790

Table 3 of 4

1 row
CharacteristicValueUnitMethod
Izod Impact Strength267J/mASTM D256

Table 4 of 4

4 rows
CharacteristicValueUnitMethod
Melt Temperature Range205 - 220°C—
Mold Temperature Range10 - 25°C—
Mold Shrinkage Rate0.6 - 0.9%ASTM D955
Pre-Drying Conditions (at 85°C)2Hours(do not over-dry)