To catalogue

Ecomass® Compound 4703ZD88

Ecomass® compound 4703ZD88 is a tungsten-filled thermoplastic polyurethane compound that is recommended to be used in weighting, balancing, radiation shielding and vibration dampening applications. This injection molding grade is known for its excellent toughness and flexibility. Additionally, it functions as a nontoxic thermoplastic lead substitute.

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Consumer Goods — Sports & Recreation
Healthcare & Pharma — Medical
  • Medical Devices & Assemblies
Electrical & Electronics — Parts & Components
  • Housings & Enclosures

Product Families

Composite Materials — Polymers & Resins
  • Thermoplastic Resins
Elastomers — Thermoplastic Elastomers
  • Thermoplastic Urethanes (TPU)

Other characteristics

Brand
Ecomass
Density
6800.0 - 6800.0 kg/m³
Polymer Name
Thermoplastic Polyurethane (unspecified)
Fillers Included
Tungsten
Processing Methods
Injection Molding, Injection Molding
Color
  • Grey
  • Opaque
Markets
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Technology
  • Composite Materials
  • Elastomers
Labeling Claims
Non-Toxic
Material Features
  • Ambient Operating Temperature
  • Excellent Toughness
  • Flexible
  • Lead Substitute
  • Low Odor
  • Non-Toxic
  • Vibration Damping
Chemical Inventories
  • AICS (Australia)
  • DSL (Canada)
  • EINECS (EU)
  • ENCS (Japan)
  • IECSC (China)
  • KECI (Korea)
  • PICCS (Phillipines)
  • TSCA (USA)
Certifications and Compliance
RoHS Compliant
Composites Processing Methods
Injection Molding
Plastics and Elastomers End Uses
  • Medical Devices
  • Radiation Shielding
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 3

1 row
CharacteristicValueUnitMethod
Density6.8g/ccASTM D792

Table 2 of 3

6 rows
CharacteristicValueUnitMethod
Tensile Elongation at Break58%ASTM D638
Tensile Strength17MPaASTM D638
Tensile Modulus662MPaASTM D638
Izod Impact Strength (notched)241J/mASTM D256
Flexural Modulus113MPaASTM D790
Flexural Strength26MPaASTM D790

Table 3 of 3

4 rows
CharacteristicValueUnitMethod
Melt Temperature Range205 - 220°C—
Mold Temperature Range10 - 25°C—
Mold Shrinkage Rate0.4 - 0.6%ASTM D955
Pre-Drying Conditions (at 85°C)2 - 4Hours(do not over-dry)