Ecomass® Compound 705ZD70
- Chemical Family
- Acrylonitrile Butadiene Styrene (ABS)Styrenics
Ecomass® compound 705ZD70 is a tungsten-filled acrylonitrile butadiene styrene compound that is recommended to be used in weighting, balancing and radiation shielding applications. This extrusion grade is known for its high specific gravity, good toughness and rigidity. Additionally, it functions as a nontoxic thermoplastic lead substitute.
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Healthcare & Pharma — Medical
- Medical Devices & Assemblies
Electrical & Electronics — Parts & Components
- Housings & Enclosures
Product Families
Plastics — Basic Thermoplastics
- Styrenics
Composite Materials — Polymers & Resins
- Thermoplastic Resins
Other characteristics
- Brand
- Ecomass
- Density
- 3000.0 - 3000.0 kg/m³
- Polymer Name
- Acrylonitrile Butadiene Styrene (ABS)
- Fillers Included
- Tungsten
- Processing Methods
- Extrusion, Injection Molding, Injection Molding
- Color
- Grey
- Markets
- Electrical & Electronics
- Healthcare & Pharma
- Technology
- Composite Materials
- Plastics
- Labeling Claims
- Non-Toxic
- Material Features
- Ambient Operating Temperature
- Good Rigidity
- Good Toughness
- Heavy Plastic
- High Density
- High Specific Gravity
- Lead Substitute
- Low Odor
- Chemical Inventories
- AICS (Australia)
- DSL (Canada)
- EINECS (EU)
- ENCS (Japan)
- IECSC (China)
- NZIoC (New Zealand)
- PICCS (Phillipines)
- TSCA (USA)
- Certifications and Compliance
- ISO 9001
- Korea Toxic Chemicals Control Act (TCCA)
- RoHS Compliant
- Composites Processing Methods
- Extrusion
- Injection Molding
- Plastics and Elastomers End Uses
- Medical Devices
- Radiation Shielding
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
- Injection Molding
Technical data
Table 1 of 5
1 row| Characteristic | Value | Unit |
|---|---|---|
| Density | 3 | g/cc |
Table 2 of 5
3 rows| Characteristic | Value | Unit |
|---|---|---|
| Tensile Elongation at Break | 3 | % |
| Tensile Strength | 30 | psi |
| Flexural Modulus | 2900 | psi |
Table 3 of 5
1 row| Characteristic | Value | Unit |
|---|---|---|
| Izod Impact Strength | 6 | ft-lb/in |
Table 4 of 5
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Temperature Range | 250 - 287 | °F | — |
| Mold Temperature Range | 35 - 65 | °F | — |
| Mold Shrinkage Rate | .4 - .6 | in/in | (4mm) |
| Pre-Drying Conditions (at 70 - 85°C) | 2 - 4 | Hours | — |
Table 5 of 5
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Temperature Range | 250 - 287 | °F | — |
| Mold Temperature Range | 35 - 65 | °F | — |
| Mold Shrinkage Rate | .4 - .6 | in/in | (4mm) |
| Pre-Drying Conditions (at 70 - 85°C) | 2 - 4 | Hours | — |