To catalogue
Ecomass® Compound 1002ZC76
- Chemical Family
- Polyamides
Ecomass® Compound 1002ZC76 is a stainless steel powder-filled polyether block amide (PEBA) compound that is flexible and exhibits excellent toughness. The processing method for this compound is injection molding/extrusion. It is a nontoxic alternative to lead (Pb) and is used for weighting and balancing applications.
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Applications
- Consumer Goods — Sports & Recreation
Electrical & Electronics — Parts & Components
- Housings & Enclosures
Product Families
Composite Materials — Polymers & Resins
- Thermoplastic Resins
Elastomers — Thermoplastic Elastomers
- Thermoplastic Polyamide Elastomers (TPE-A)
Other characteristics
- Brand
- Ecomass
- Density
- 3000.0 - 3000.0 kg/m³
- Polymer Name
- Polyether Block Amide (PEBA)
- Fillers Included
- Stainless Steel Powder
- Processing Methods
- Extrusion, Injection Molding, Injection Molding
- Markets
- Consumer Goods
- Electrical & Electronics
- Technology
- Composite Materials
- Elastomers
- Labeling Claims
- Non-Toxic
- Material Features
- Excellent Toughness
- Flexible
- Hot Operating Temperature
- Lead Substitute
- Low Odor
- Medium Density
- Non-Toxic
- Chemical Inventories
- AICS (Australia)
- DSL (Canada)
- EINECS (EU)
- ENCS (Japan)
- IECSC (China)
- ISHL (Japan)
- KECI (Korea)
- PICCS (Phillipines)
- Certifications and Compliance
- RoHS Compliant
- Composites Processing Methods
- Extrusion
- Injection Molding
- Plastics and Elastomers End Uses
- Casino Chips
- Frangible Projectiles
- Golf Club Weights
- Hub Odometer
- Inertia Discs
- Instrument Housing
- Manual Transmission Shifter Cartridge
- Return Weights
- Plastics and Elastomers Processing Methods
- Extrusion
- Injection Molding
Technical data
Table 1 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 3 | g/cc | Internal |
Table 2 of 4
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength | 4 | MPa | ISO 527 |
| Tensile Elongation at Yield | 160 | % | ISO 527 |
| Izod Impact Strength, Notched | 9.3 | KJ/m | ISO 180/A |
Table 3 of 4
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Temperature Range | 230 - 260 | °C | — |
| Mold Temperature Range | 65 - 80 | °C | — |
| Mold Shrinkage Rate | 0.2 - 0.4 | % | Internal |
| Pre-Drying Conditions (at 80°C) | 4 - 6 | hrs | Target moisture max. 0.20% |
Table 4 of 4
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Temperature Range | 230 - 260 | °C | — |
| Mold Temperature Range | 65 - 80 | °C | — |
| Mold Shrinkage Rate | 0.2 - 0.4 | % | Internal |
| Pre-Drying Conditions (at 80°C) | 4 - 6 | hrs | Target moisture max. 0.20% |