To catalogue
Ecomass® Compound 4150ZC78
- Chemical Family
- Polyphenylene Sulfide (PPS)
Ecomass® Compound 4150ZC78 is a filled polyphenylene sulfide (PPS) compound used in various applications. The compound is specifically designed for injection molding, making it ideal for manufacturing processes requiring this method. It is supplied in the form of pellets, facilitating easy handling and seamless integration into the production process.
Properties
- Physical Form
- Pellets
- Solid
Product families
Plastics — Engineering & Specialty Polymers
- High Performance Thermoplastics
Composite Materials — Polymers & Resins
- Thermoplastic Resins
Other characteristics
- Brand
- Ecomass
- Density
- 3800.0 - 3800.0 kg/m³
- Polymer Name
- Polyphenylene Sulfide (PPS)
- Fillers Included
- Stainless Steel Fiber
- Processing Methods
- Injection Molding, Injection Molding
- Technology
- Composite Materials
- Plastics
- Material Features
- Filled
- Heavy Plastic
- Hot Operating Temperature
- Medium Density
- Certifications and Compliance
- RoHS Compliant
- Composites Processing Methods
- Injection Molding
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 3.8 | g/cc | ASTM D792 |
Table 2 of 4
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength | 34 | MPa | ASTM D638 |
| Tensile Modulus | 3448 | MPa | ASTM D638 |
| Tensile Elongation at Break | 3 | % | ASTM D638 |
| Flexural Modulus | 3448 | MPa | ASTM D790 |
| Flexural Strength | 41 | MPa | ASTM D790 |
| Izod Impact Strength, Notched | 48 | J/m | ASTM D256 |
Table 3 of 4
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Heat Deflection Temperature (at 66 psi) | 135 | °C | ASTM D648 |
| Heat Deflection Temperature (at 264 psi) | 127 | °C | ASTM D648 |
Table 4 of 4
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Temperature Range | 315 - 345 | °C | — |
| Mold Temperature Range | 135 - 150 | °C | — |
| Mold Shrinkage Rate | 0.8 - 1.0 | % | ASTM D955 |
| Pre-Drying Conditions (at 120°C) | 4 | hrs | — |