To catalogue
Ecomass® Compound 1850IO43T1 Natural
- Chemical Family
- Polyamides
Ecomass® Compound 1850IO43T1 Natural is an iron oxide-filled polyamide 6 (PA6) compound that is impact-modified. The processing method for this compound is injection molding. It is a nontoxic alternative to lead (Pb) and is used for weighting and balancing applications.
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Applications
- Consumer Goods — Sports & Recreation
Electrical & Electronics — Parts & Components
- Housings & Enclosures
Product Families
Plastics — Engineering & Specialty Polymers
- Polyamides
Composite Materials — Polymers & Resins
- Thermoplastic Resins
Other characteristics
- Brand
- Ecomass
- Density
- 1700.0 - 1700.0 kg/m³
- Polymer Name
- Polyamide 6 (PA 6)
- Fillers Included
- Iron Oxide
- Processing Methods
- Injection Molding, Injection Molding
- Markets
- Consumer Goods
- Electrical & Electronics
- Technology
- Composite Materials
- Plastics
- Labeling Claims
- Non-Toxic
- Material Features
- Ambient Operating Temperature
- Heavy Plastic
- Impact Modified
- Medium Density
- Non-Toxic
- Certifications and Compliance
- RoHS Compliant
- Composites Processing Methods
- Injection Molding
- Plastics and Elastomers End Uses
- Casino Chips
- Frangible Projectiles
- Golf Club Weights
- Hub Odometer
- Inertia Discs
- Instrument Housing
- Manual Transmission Shifter Cartridge
- Return Weights
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1.7 | g/cc | Internal |
Table 2 of 4
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength | 57 | psi | ISO 527 |
| Tensile Elongation at Break | 8 | % | ISO 527 |
| Flexural Modulus | 2900 | psi | ISO 178 |
| Izod Impact Strength, Notched | 7.4 | ft-lb/in | ISO 180/A |
Table 3 of 4
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Heat Deflection Temperature (at 66 psi) | 150 | °F | ASTM D648 |
| Heat Deflection Temperature (at 264 psi) | 50 | °F | ASTM D648 |
Table 4 of 4
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Temperature Range | 255 - 290 | °F | — |
| Mold Temperature Range | 65 - 85 | °F | — |
| Mold Shrinkage Rate | 0.7 - 0.9 | in/in | Internal |
| Pre-Drying Conditions (at 80°C) | 4 - 6 | hrs | Target moisture max. 0.20% |