LNP™ THERMOCOMP™ Compound OF008G
- Chemical Family
- Polyphenylene Sulfide (PPS)
LNP THERMOCOMP OF008G compound is based on linear Polyphenylene Sulfide (PPS) resin containing 15% glass fiber, 25% milled glass.
Product families
Applications
- Consumer Goods — Appliances & Electronics
- Consumer Goods — Lawn & Garden
- Consumer Goods — Sports & Recreation
- Artificial Turf
- Consumer Electronics
- Displays
- Non-Food Consumer Packaging
- Applicators & Accessories
- Connectors
- Housings & Enclosures
- Switches & Relays
Product Families
- High Performance Thermoplastics
Other characteristics
- Brand
- LNP™ THERMOCOMP™ Compound
- Polymer Name
- Polyphenylene Sulfide (PPS)
- Fillers Included
- Glass Fiber, Milled Glass Fiber
- Glass Fiber
- Milled Glass Fiber
- Processing Methods
Fused Deposition Modeling (FDM), Injection Molding
- Note
ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.; ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.; ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
- Markets
- Building & Construction
- Consumer Goods
- Electrical & Electronics
- Personal Care
- Printing & Packaging
- Technology
- Plastics
- Material Features
- Cost Effective
- High Linearity
- High Modulus
- High Stiffness
- Country Availability
- Canada
- China (Mainland)
- Mexico
- USA
- Plastics and Elastomers End Uses
- Appliances
- Building Materials
- Cell Phones
- Commercial Appliance
- Computer Components
- Consumer Applications
- Containers
- Displays
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Fused Deposition Modeling (FDM)
- Injection Molding
Technical data
Table 1 of 4
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Stress (Break, Type I, 5 mm/min) ¹¹ | 104 | MPa | ASTM D638 |
| Tensile Strain (Break, Type I, 5 mm/min) ¹¹ | 1.9 | % | ASTM D638 |
| Tensile Modulus (at 5 mm/min) ¹¹ | 8840 | MPa | ASTM D638 |
| Flexural Stress (Break, 1.3 mm/min, 50 mm span) ¹¹ | 157 | MPa | ASTM D790 |
| Flexural Modulus (at 1.3 mm/min, 50 mm span) ¹¹ | 9300 | MPa | ASTM D790 |
Table 2 of 4
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Mold Shrinkage (flow, 24 hrs) ᵍ ¹¹ | 0.2 - 0.5 | % | ASTM D955 |
| Mold Shrinkage (xflow, 24 hrs) ᵍ ¹¹ | 0.8 - 1 | % | ASTM D955 |
Table 3 of 4
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Izod Impact (Unnotched, at 23°C) ¹¹ | 395 | J/m | ASTM D4812 |
| Izod Impact (Notched, at 23°C) ¹¹ | 68 | J/m | ASTM D256 |
Table 4 of 4
9 rows| Characteristic | Value | Unit |
|---|---|---|
| Drying Temperature ⁷ | 120 - 150 | °C |
| Drying Time ⁷ | 4 | Hrs |
| Melt Temperature ⁷ | 315 - 320 | °C |
| Front - Zone 3 Temperature ⁷ | 330 - 345 | °C |
| Middle - Zone 2 Temperature ⁷ | 320 - 330 | °C |
| Rear - Zone 1 Temperature ⁷ | 305 - 315 | °C |
| Mold Temperature ⁷ | 140 - 165 | °C |
| Back Pressure ⁷ | 0.2 - 0.3 | MPa |
| Screw Speed ⁷ | 30 - 60 | rpm |