NORYL™ Resin PX2938
SABIC's Specialties Business NORYL PX2938 resin is a 20% glass fiber reinforced blend of polyphenylene ether (PPE) + polystyrene (PS). This injection molding and extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 at 0.75mm. NORYL PX2938 resin exhibits high heat resistance, high impact strength, dimensional stability, hydrolytic stability, and very low moisture absorption. This material is an excellent candidate for industrial applications such as cooling fans. This product does not contain PFAS intentionally added during SHPP’s manufacturing process and are not expected to contain unintentional PFAS impurities. Each user is responsible for evaluating the presence of unintentional PFAS impurities.
Product families
Applications
- Consumer Goods — Appliances & Electronics
- Glazing & Window Elements
- Interior Fixtures
- Pipes & Plumbing
- Consumer Electronics
- Displays
- Medical Devices & Assemblies
- Connectors
- Switches & Relays
Product Families
- Blends & Alloys
Other characteristics
- Brand
- NORYL™ Resin
- Density
- 1260.0 - 1260.0 kg/m³
- Polymer Name
- PPO/PS Alloy
- Flexural Modulus
- 5640.0 - 5640.0 MPa
- Processing Methods
- Injection Molding
- Note
ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.; ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.; ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
- Markets
- Building & Construction
- Consumer Goods
- Electrical & Electronics
- Healthcare & Pharma
- Flame Rating
- UL 94 V0
- Technology
- Plastics
- Labeling Claims
- Bromine-free
- Chlorine-free
- No Added PFAS
- Fillers Included
- Glass Fiber
- Additives Included
- Flame Retardant
- Material Features
- Amorphous
- Dimensional Stability
- Flame Retardant
- Good Stiffness
- High Hydrolytic Stability
- High Stiffness
- High Strength
- Low Moisture Absorption
- Country Availability
- China (Mainland)
- Certifications and Compliance
- UL 94
- Plastics and Elastomers End Uses
- Building Materials
- Cell Phones
- Computer Components
- Construction Applications
- Displays
- Electrical Components
- Electrical/Electronic Applications
- Faucet System Components
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 5
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Stress (Yield) ¹¹ | 107 | MPa | SABIC - Japan Method |
| Tensile Strain (Break) ¹¹ | 8 - 8 | % | SABIC - Japan Method |
| Flexural Stress ¹¹ | 143 | MPa | ASTM D790 |
| Flexural Modulus ¹¹ | 5640 | MPa | ASTM D790 |
| Hardness (Rockwell R) ¹¹ | 127 | — | ASTM D785 |
Table 2 of 5
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Specific Gravity ¹¹ | 1.26 | — | ASTM D792 |
| Water Absorption (at 23°C, 24hrs) ¹¹ | 0.06 | % | ASTM D570 |
| Mold Shrinkage (flow, 3.2 mm) ᵍ ¹¹ | 0.2 - 0.4 | % | SABIC method |
| Melt Flow Rate (at 300°C, 5.0 kgf) ¹¹ | 19.8 | g/10 min | ASTM D1238 |
Table 3 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Heat Deflection Temperature (at 1.82 MPa, 6.4 mm, Unannealed) ¹¹ | 143 | °C | ASTM D648 |
| Coefficient of Thermal Expansion (at -30°C to 30°C) ¹¹ | 0.000027 - 0.000044 | 1/°C | TMA |
Table 4 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Izod Impact (Notched, at 23°C) ¹¹ | 87 | J/m | ASTM D256 |
| Izod Impact (Notched, at -30°C) ¹¹ | 85 | J/m | ASTM D256 |
Table 5 of 5
13 rows| Characteristic | Value | Unit |
|---|---|---|
| Drying Temperature ⁷ | 110 - 120 | °C |
| Drying Time ⁷ | 3 - 4 | Hrs |
| Drying Time (Cumulative) ⁷ | 8 | Hrs |
| Maximum Moisture Content ⁷ | 0.02 | % |
| Melt Temperature ⁷ | 300 - 325 | °C |
| Nozzle Temperature ⁷ | 300 - 325 | °C |
| Front - Zone 3 Temperature ⁷ | 290 - 325 | °C |
| Middle - Zone 2 Temperature ⁷ | 275 - 320 | °C |
| Rear - Zone 1 Temperature ⁷ | 265 - 315 | °C |
| Mold Temperature ⁷ | 80 - 110 | °C |
| Back Pressure ⁷ | 0.3 - 0.7 | MPa |
| Screw Speed ⁷ | 20 - 100 | rpm |