To catalogue

NORYL™ Resin 115EM4

NORYL 115EM4 compound is based on Polyphenylene Ether (PPE) resin containing conductive carbon powder and minerals. Added features of this grade include: Electrically Conductive.

Product families

Applications

Industrial — Chemical & Industrial Manufacturing
  • Equipment & Parts
Electrical & Electronics — Devices & Assemblies
  • Industrial Automation
Electrical & Electronics — Parts & Components
  • Semiconductor Manufacturing

Product Families

Plastics — Engineering & Specialty Polymers
  • Blends & Alloys

Other characteristics

Brand
NORYL™ Resin
Density
1160.0 - 1160.0 kg/m³
Polymer Name
PPO/PS Alloy
Flexural Modulus
3340.0 - 3340.0 MPa
Processing Methods
Injection Molding
Note

ᵈ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding. Do NOT mix NORYL GTX* resin with other grades of NORYL* resins. Polystyrene and acrylic regrind are effective purging Materials. Use temperature range appropriate for particular purging resin. Regrind must also be dried. Maximum 25% regrind. Dry at recommended temperatures and times for optimum performance. Overdrying can cause loss of physical properties and/or create appearance defects. Do not exceed recommended basic drying time and temperature above or:\n4-8 hrs at 95°C (200°F), 10 hrs max\n6-12 hrs at 80°C (175°F), 16 hrs max\n8-16 hrs at 65°C (150°F), 24 hrs max\nAVOID air circulating tray ovens. Moisture levels in heated ambient air can exceed moisture level in the resin itself, causing moisture ABSORPTION not drying. Avoid melt temperature in excess of 300°C (575°F) and residence times over 6-8 minutes (may affect properties and/or appearance). Nozzle temperature controls assist in elimination of drool premature freeze-off. Shot sizes in excess of 50% barrel capacity can lead to difficulties in providing a consistent, homogenous plastic melt.; ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.; ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.; ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.

Markets
  • Electrical & Electronics
  • Industrial
Technology
Plastics
Fillers Included
  • Carbon Black
  • Carbon Powder
  • Mineral
  • Talc
Additives Included
  • Heat Stabilizer
  • Impact Modifier
  • Mold Release Agent
Material Features
  • Electrically Conductive
  • Good Mold Release
  • Heat Stabilized
  • Impact Modified
Country Availability
  • Canada
  • China (Mainland)
  • Mexico
  • USA
Plastics and Elastomers End Uses
  • Computer Components
  • Electrical/Electronic Applications
  • Electronic Components
  • Industrial Applications
  • Semiconductor Applications
  • Trays
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 6

4 rows
CharacteristicValueUnitMethod
Tensile Stress (Yield) ¹¹69MPaSABIC - Japan Method
Tensile Strain (Break) ¹¹6%SABIC - Japan Method
Flexural Stress ¹¹108MPaASTM D790
Flexural Modulus ¹¹3340MPaASTM D790

Table 2 of 6

2 rows
CharacteristicValueUnitMethod
Specific Gravity ¹¹1.16—ASTM D792
Mold Shrinkage (flow, 3.2 mm) ᵍ ¹¹0.7 - 0.8%SABIC method

Table 3 of 6

1 row
CharacteristicValueUnitMethod
Heat Deflection Temperature (at 0.45 MPa, 3.2 mm, Unannealed) ¹¹163°CASTM D648

Table 4 of 6

1 row
CharacteristicValueUnitMethod
Surface Resistivity ᵈ ¹¹10000 - 1000000ΩASTM D257

Table 5 of 6

1 row
CharacteristicValueUnitMethod
Izod Impact (Notched, at 23°C) ¹¹49J/mASTM D256

Table 6 of 6

12 rows
CharacteristicValueUnit
Back Pressure (Plastic Pressure) ⁷5 - 10MPa
Drying Temperature ⁷100°C
Drying Time ⁷3 - 5Hrs
Front - Zone 3 Temperature ⁷290 - 320°C
Maximum Moisture Content ⁷0.02%
Melt Temperature ⁷290 - 320°C
Middle - Zone 2 Temperature ⁷280 - 310°C
Mold Temperature ⁷80 - 120°C
Nozzle Temperature ⁷285 - 315°C
Rear - Zone 1 Temperature ⁷270 - 300°C
Screw Speed (Circumferential speed) ⁷0.1 - 0.2m/s
Shot to Cylinder Size ⁷30 - 70%