LNP™ ELCRIN™ 610001UXiQ
SABIC's Specialties Business LNP ELCRIN 610001UXiQ compound is based on Polycarbonate / Polybutylene Terephthalate (PC/PBT) blend, utilizing ELCRIN iQ upcycling technology containing minimum 12% Post-Consumer Recycling (PCR) weight content. Added features of this grade include: Non-Chlorinated, Non-Brominated Flame Retardant, Good Flow, High Impact, Improved Chemical Resistance, UV Resistant.
Other characteristics
- Brand
- LNP™ ELCRIN
- Density
- 1200.0 - 1200.0 kg/m³
- Polymer Name
- PC/PBT Alloy
- Labeling Claims
Bromine-free, Chlorine-free, Contains PCR Resin, Recyclable, Recycled, Sustainable; Bromine-free; Chlorine-free; Contains PCR Resin; Recyclable; Recycled; Sustainable
- Melt Flow Index
- 26.0 - 26.0 g/10 min
- Processing Methods
- Injection Molding
- Note
ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.; ᵖ UL ratings shown on the technical datasheet might not cover the full range of thicknesses and colors. For details, please see the UL Yellow Card.; ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.; ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
- Markets
- Automotive & Transportation
- Consumer Goods
- Electrical & Electronics
- Healthcare & Pharma
- Personal Care
- Printing & Packaging
- Flame Rating
- UL 94 5VB
- UL 94 V0
- UL 94 V1
- Technology
- Plastics
- Additives Included
- Flame Retardant
- Material Features
- Chemical Resistant
- Flame Retardant
- Good Flow
- Good UV Stability
- Good Weather Stability
- High Flow
- High Flowability
- High Impact Performance
- Country Availability
- Canada
- China (Mainland)
- Mexico
- USA
- Certifications and Compliance
- UL 94
- Plastics and Elastomers End Uses
- Automotive Applications
- Automotive Interior Parts
- Cell Phones
- Clinical Diagnostics
- Computer Components
- Connectors
- Consumer Applications
- Containers
- Plastics and Elastomers Functions
- Resin
Technical data
Table 1 of 6
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Stress (Yield, Type I, 50 mm/min) ¹¹ | 63 | MPa | ASTM D638 |
| Tensile Stress (Break, Type I, 50 mm/min) ¹¹ | 42 | MPa | ASTM D638 |
| Tensile Strain (Yield, Type I, 50 mm/min) ¹¹ | 4 | % | ASTM D638 |
| Tensile Strain (Break, Type I, 50 mm/min) ¹¹ | 65 | % | ASTM D638 |
| Tensile Modulus (at 50 mm/min) ¹¹ | 2480 | MPa | ASTM D638 |
| Flexural Stress (Yield, 1.3 mm/min, 50 mm span) ¹¹ | 89 | MPa | ASTM D790 |
| Flexural Modulus (at 1.3 mm/min, 50 mm span) ¹¹ | 2240 | MPa | ASTM D790 |
Table 2 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Specific Gravity ¹¹ | 1.2 | — | ASTM D792 |
| Mold Shrinkage (flow, 3.2 mm) ᵍ ¹¹ | 0.5 - 0.7 | % | SABIC method |
| Melt Flow Rate (at 266°C, 5.0 kgf) ¹¹ | 26 | g/10 min | ASTM D1238 |
Table 3 of 6
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Heat Deflection Temperature (at 1.82 MPa, 3.2mm, Unannealed) ¹¹ | 77 | °C | ASTM D648 |
| Vicat Softening Temperature (Rate B/50) ¹¹ | 100 | °C | ASTM D1525 |
| Relative Temperature Index (Electrical) ᵖ ¹¹ | 75 | °C | UL 746B |
| Relative Temperature Index (Mechanical with impact) ᵖ ¹¹ | 75 | °C | UL 746B |
| Relative Temperature Index (Mechanical without impact) ᵖ ¹¹ | 75 | °C | UL 746B |
Table 4 of 6
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Izod Impact (Notched, at 23°C) ¹¹ | 550 | J/m | ASTM D256 |
| Instrumented Dart Impact Total Energy (at 23°C) ¹¹ | 65 | J | ASTM D3763 |
Table 5 of 6
14 rows| Characteristic | Value | Unit |
|---|---|---|
| Drying Temperature ⁷ | 80 - 90 | °C |
| Drying Time ⁷ | 3 - 4 | Hrs |
| Drying Time (Cumulative) ⁷ | 8 | Hrs |
| Maximum Moisture Content ⁷ | 0.04 | % |
| Melt Temperature ⁷ | 245 - 275 | °C |
| Nozzle Temperature ⁷ | 245 - 275 | °C |
| Front - Zone 3 Temperature ⁷ | 245 - 275 | °C |
| Middle - Zone 2 Temperature ⁷ | 220 - 265 | °C |
| Rear - Zone 1 Temperature ⁷ | 220 - 255 | °C |
| Mold Temperature ⁷ | 60 - 80 | °C |
| Back Pressure ⁷ | 0.3 - 0.7 | MPa |
| Screw Speed ⁷ | 40 - 70 | rpm |
Table 6 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| UL Recognized (94V-1 Flame Class Rating) ᵖ | min. 1.1 | mm | UL 94 |
| UL Recognized (94V-0 Flame Class Rating) ᵖ | min. 1.5 | mm | UL 94 |
| UL Recognized (94-5VB Flame Class Rating) ᵖ | min. 2.5 | mm | UL 94 |