Aegis® H120ZP resin is a high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film applications. It combines strength, toughness and thermoforming properties with excellent heat, chemical and abrasion resistance.

Product families

Applications

Applications
  • Consumer Goods — Other Consumer Goods Applications; Consumer Goods — Sports & Recreation
Printing & Packaging — Packaging
  • Food & Beverage Packaging
  • Industrial & Transport Packaging
Food & Nutrition — Processing & Packaging
  • Food & Beverage Packaging

Product Families

Plastics — Engineering & Specialty Polymers
  • Polyamides

Other characteristics

Brand
Aegis®
Polymer Name
Polyamide 6 (PA 6)
Processing Methods
Extrusion
Markets
  • Consumer Goods
  • Food & Nutrition
  • Healthcare & Pharma
  • Printing & Packaging
Technology
Plastics
Extrusion Guidelines

Melt Viscosity vs. Temperature; Melt Temperature: 220°C (428°F) Melt Temperature Range: 232°C (450°F) to 271°C (520°F). Two key factors affect the melt viscosity (stiffness or fluidity of the melt):; The molecular weight (Mw) of the resin: Higher Mw resins will have a higher melt viscosity than lower Mw resins.; Temperature of the melt for any given Mw resin: Higher process temperatures will provide a more fluid melt viscosity than lower process temperatures.; Typical Barrel Profile for Cast Films; Barrel: 230-260°C (446-500°F) Adapter: 260-266°C (500-510°F) Die: 260°C (500°F) Process Melt Temperature: 260-270°C (500-518°F); Typical Barrel Profile for Tubular (Blown) Films; Barrel: 246-254°C (474-490°F) Adapter: 260°C (500°F) Die: 254°C (490°F) Process Melt Temperature: 254-260°C (490-500°F); Screw Parameters; Metering Section: 40% Transition Section: 3 to 4 flights Feed Section: Balance of screw length Compression Ratio: 3.5:1 to 4.0:1 L/D Ratio: 24:1; Metering Section Flight Depth

Processing Guidelines

Material Handling. Aegis® H120ZP homopolymer is supplied in sealed containers and drying prior to processing is not required. However, high moisture is the primary cause of processing problems. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 80°C (176°F) is recommended. Drying time is dependent on moisture level.

Regulatory Compliance

AdvanSix has more than 50 years of experience in the development and production of packaging resin that is safe and reliable for consumers and businesses. Aegis® packaging resins are manufactured to meet the stringent standards required of materials involved in the processing, handling and packaging of food. They meet all applicable U.S. Food and Drug Administration (FDA) and European Union (EU) food grade regulations, as outlined in FDA 21 CFR 177.1500 and Regulation (EU) No. 10/2011.

Plastics and Elastomers End Uses
  • Balloons
  • Book Covers
  • Fans
  • Film
  • Flexible Packaging
  • Food Packaging
  • Form Fill Seal Packaging
  • Front Spoiler
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Extrusion

Technical data

Table 1 of 2

10 rows
CharacteristicValueUnitMethod
Viscosity FAV120—ASTM D-789
RV (at 96% Sulfuric Acid)3.6——
Extractable Contentmax. 0.8%SOP-702-307
Density1.13g/cm3ASTM D-792
Melt Flow Rate (at 235°C/1.0 kg (455°F/1.0 kg))1.9g/10 minASTM D-1238
Moisture Contentmax. 0.08%ASTM D-6869
Moisture (24 Hour)1.6%ASTM D-570
Moisture (50% RH)2.7%ASTM D-570
Moisture (Saturation)9.5%ASTM D-570
Melting Point220 (428)°C (°F)ASTM D-3418

Table 2 of 2

4 rows
CharacteristicValueUnitMethod
Oxygen Permeability (at 23°C (73°F)/0% RH)40.3 (2.6)cc.25μm/m²/day (cc.mil/100 in²/day)D-3958
Water Vapor Permeability (at 38°C (100°F)/100% RH)992 (64)gm.25μm/m²/day (gm.mil/100 in²/day)F-1249
Nitrogen Permeability (at 23°C (73°F)/0% RH)14.0 (0.9)cc.25μm/m²/day (cc.mil/100 in²/day)—
Carbon Dioxide Permeability72.8 (4.7)cc.25μm/m²/day (cc.mil/100 in²/day)—