OPTIM® E-126

OPTIM® E-126 is a maleic anhydride modified linear low density polyethylene. It is used for toughening of Polyamides such as Nylon-6 & Nylon 6, 6.

Properties

Physical Form
  • Masterbatch
  • Solid

Product families

Applications

Electrical & Electronics — Wire & Cable
  • Jacketing & Insulation

Product Families

Plastics — Masterbatches
  • Additive Masterbatches
Plastics — Polymer Additives
  • Performance Additives
  • Surface Modifiers

Other characteristics

Brand
OPTIM
Carrier

Linear Low Density Polyethylene (LLDPE), Resin-based; Linear Low Density Polyethylene (LLDPE); Resin-based

Features
Good Adhesion, Non-Hygroscopic
Functions
Compatibilizer, Coupling Agent, Impact Modifier
Compatible Polymers & Resins
Polyamide 6 (PA 6), Polyamide 66 (PA 66)
Markets
Electrical & Electronics
Technology
Plastics
Packaging Type
  • Bags
  • Super Sacks
Material Features
  • Good Adhesion
  • Non-Hygroscopic
Packaging Information

OPTIM® speciality polymers are supplied in pre-dried form in 25 Kg (55 lbs) PE lined, HD woven sack-laminated paper bags and 750 Kg (1650 lbs) FIBC's.. They should be stored in cool and dry place.

Processing Conditions

OPTIM® E-126 can be added to Polyamides to achieve good dispersion of fillers within the polymer matrix thereby obtaining best properties.; Maximum processing temperature should not generally exceed 290°C.; At temperatures above 290°C, these speciality polymers can evolve low concentrations of fumes.; If overheated, more extensive decomposition may occur due to exposure of overheated polymers to atmospheric oxygen.; Adequate local ventilation should be provided to remove the fumes from the work area.

Compatible Polymers and Resins
  • Polyamide 6 (PA 6)
  • Polyamide 66 (PA 66)
Plastics and Elastomers End Uses
  • Cables
  • Wires
Plastics and Elastomers Functions
  • Compatibilizer
  • Coupling Agent
  • Impact Modifier
Storage and Handling Procedures

OPTIM® E-126 should be stored in a dry, cool and well-ventilated area.. It is recommended that prior to processing, the requisite quantity of material to be used should be dried in a hopper dryer or oven at 80-95°C for about 2 hours for obtaining best results.

Technical data

Table 1 of 4

5 rows
CharacteristicValueUnitMethod
Tensile Strength15MPaASTM D638/2010
Percentage Elongation31%ASTM D638/2010
Tensile Modulus170MPaASTM D638/2010
Flexural Modulus360MPaASTM D790/2010
Flexural Strength13MPaASTM D790/2010

Table 2 of 4

2 rows
CharacteristicValueUnitMethod
Melting Temperature125°CDSC
Vicat Softening Temperature119°CASTM 1525/2010

Table 3 of 4

4 rows
CharacteristicValueUnitMethod
MFI (at 190°C/2.16 Kg)0.6g/10minASTM D1238
Density0.931g/cm³ASTM D792
Bulk Density0.54g/mlPLUSS® method
Bonded Maleic AnhydrideMedium—PLUSS® method

Table 4 of 4

1 row
CharacteristicValueUnitMethod
Durometer Hardness58Shore DASTM D2240/2004