OPTIM® E-142
OPTIM® E-142 is a maleic anhydride modified linear low density polyethylene. It is used for toughening of Polyamides such as Nylon-6.
Properties
- Physical Form
- Masterbatch
- Solid
Product families
Applications
- Jacketing & Insulation
Product Families
- Additive Masterbatches
- Performance Additives
Other characteristics
- Brand
- OPTIM
- Carrier
- Low-Density Polyethylene (LDPE), Resin-based
- Low-Density Polyethylene (LDPE)
- Resin-based
- Features
- Good Adhesion, Non-Hygroscopic
- Functions
- Compatibilizer, Impact Modifier
- Compatible Polymers & Resins
Polyamide 6 (PA 6), Polyamides, Polyethylenes (PE)
- Markets
- Electrical & Electronics
- Technology
- Plastics
- Packaging Type
- Bags
- Super Sacks
- Material Features
- Good Adhesion
- Non-Hygroscopic
- Packaging Information
OPTIM® speciality polymers are supplied in pre-dried form in 25 Kg (55 lbs) PE lined, HD woven sack-laminated paper bags and 750 Kg (1650 lbs) FIBC's.. They should be stored in cool and dry place.
- Processing Conditions
OPTIM® E-142 can be added to nylons to achieve good dispersion of fillers within the polymer matrix thereby obtaining best properties.; Maximum processing temperature should not generally exceed 290°C.; At temperatures above 290°C, these specialty polymers can evolve low concentrations of fumes.; If overheated, more extensive decomposition may occur due to exposure of overheated polymers to atmospheric oxygen.; Adequate local ventilation should be provided to remove the fumes from the work area under such conditions.
- Compatible Polymers and Resins
- Polyamide 6 (PA 6)
- Polyamides
- Polyethylenes (PE)
- Plastics and Elastomers End Uses
- Cables
- Plastics and Elastomers Functions
- Compatibilizer
- Impact Modifier
- Storage and Handling Procedures
OPTIM® E-142 should be stored in a dry, cool and well-ventilated area.. It is recommended that prior to processing, the requisite quantity of material to be used should be dried in a hopper dryer or oven at 80-95 °C for about 2 hours for obtaining best results.
Technical data
Table 1 of 4
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength | 11 | MPa | ASTM D638/2010 |
| Percentage Elongation | 150 | % | ASTM D638/2010 |
| Tensile Modulus | 30 | MPa | ASTM D638/2010 |
| Flexural Modulus | 310 | MPa | ASTM D790/2010 |
| Flexural Strength | 10 | MPa | ASTM D790/2010 |
Table 2 of 4
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melting Temperature | 116 | °C | DSC |
| Vicat Softening Temperature | 86 | °C | ASTM 1525/2010 |
Table 3 of 4
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| MFI (at 190°C/2.16 Kg) | 5 | g/10min | ASTM D1238 |
| Density | 0.923 | g/cm³ | ASTM D792 |
| Bulk Density | 0.5 | g/ml | PLUSS® method |
| Bonded Maleic Anhydride | Medium | — | PLUSS® method |
Table 4 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Durometer Hardness | 44 | Shore D | ASTM D2240/2004 |