Crown & Bridge RAYDENT® C&B
3DMaterials® Crown & Bridge RAYDENT® C&B is a biocompatible Class IIa resin for the accurate 3D printing of crowns and bridges for temporary use. Full crowns or multi-unit bridges can be printed with abrasion resistance. 3DM® C&B can be cemented with conventional cement resins C&B resin is characterized by its abrasion resistance makes 3DM® C&B suitable for this application. The waterwashable and low viscosity 3DM® C&B allows for quick and easy cleanup of the crown & bridge. A1, A2, A3 shades are available
Product families
Applications
- Dental
- Digital Printing
Product Families
- Photoactive Resins
Other characteristics
- Brand
- Crown & Bridge RAYDENT
- End Uses
- Dental Applications
- Polymer Name
- Thermoplastic (unspecified)
- Processing Methods
- 3D Printing
- Markets
- Healthcare & Pharma
- Printing & Packaging
- Technology
- Plastics
- Packaging Type
- Bottles
- Color Available
- A1, A2, A3
- Labeling Claims
- Biocompatible
- Material Features
- Abrasion Resistant
- Biocompatible
- Good Smoothness
- HIGHLIGHTS
Precise resin for printing temporary crowns and bridges. Class IIa biocompatibility makes it safe for contact with a human body lasting for up to 30 days. It's available in an A2 shade. Dental crowns and bridges made with Raydent Crown&Bridge Resin can be printed in one go or in multiple parts that have to be cemented. The resin is highly resistant to abrasion which allows the models to keep smooth surfaces and anatomical shape over the entire period of intended use. All prints must be sterilized prior to intraoral use.; A temporary dental crown.; A temporary dental crown in shade A2 printed with Raydent Crown & Bridge Resin on Zortrax Inkspire 3D printer.; Class IIa biocompatibility; Raydent Crown & Bridge resin is certified safe for continuous intraoral use lasting for up to 30 days. It's long enough to have permanent crowns and bridges made.; Abrasion-resistance; Crowns and bridges printed with Raydent Crown & Bridge Resin are highly resistant to abrasion, so they retain their shape throughout the entire period of use.; Ease of assembly; Components printed with Raydent Crown & Bridge Resin can be assembled through cementing to smooth out the joints in the structure.
- Plastics and Elastomers End Uses
- Dental Applications
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- 3D Printing
Technical data
Table 1 of 1
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Flexural Strength | min. 140 | MPa | ISO 10477 |
| Hardness | min. 90 | Shore D | ISO 178 |
| Flexural Modulus | min. 2500 | MPa | ISO 10477 |
| Sorption | max. 30 | ug/mm3 | ISO 10477 |
| Solubility | max. 10 | ug/mm3 | ISO 10477 |
| Elongation (Break) | max. 3.5 | % | ISO D638M |