G&E Blended Bromobutyl is produced by carefully combining selected feedstocks for uniform viscosity and rheology. G&E Blended Bromobutyl is excellent for cost reduction in applications such as innerliners and most mechanical goods when blended with prime Bromobutyl.

Properties

Physical Form
Solid

Product families

Applications

Industrial — Chemical & Industrial Manufacturing
  • Other Industrial Applications

Product Families

Elastomers — Thermoplastic Elastomers
  • Elastomer Blends

Other characteristics

Brand
G&E
Polymer Name
Bromobutyl Rubber (BIIR)
Markets
Industrial
PACKAGING

Thirty-six, 75 lb. (34 kg.) bales wrapped in low-melt polyethylene film are packaged in Returnable Metal Boxes weighing 2,700 lbs (1.23 MT) each. Corrugated Boxes are available with a weight of 2200 lbs (1 MT).

Technology
Elastomers
Packaging Type
  • Bales
  • Boxes

Technical data

Table 1 of 1

12 rows
CharacteristicValueUnitMethod
MOONEY VISCOSITY ML 1+8 at125°C (257°F)35 ± 10—ASTM D 1646
MOONEY VISCOSITY Raw Polymer specific Gravity0.93—ASTM F 970
MOONEY VISCOSITY (XRF Bromine Content)1.40-2.60%(G&E Method)
MOONEY VISCOSITY ( % Ash Content)Max. 2wt%ASTM D 5667 -95
MOONEY VISCOSITY (Volatile Matter, % weight)Max. 1wt%ASTM D 5668
Tensile (Cured 40 Min at 150°C(302°F))1150-2500—ASTM D 412
Elongation (Cured 40 Min at 150°C(302°F))325-525—ASTM D 412
300 % Modulus (Cured 40 Min at 150°C(302°F))500-1675—ASTM D 412
G&E Blended IIR (Internal Mixer Method)100pts.ASTM D 3958-06 (2011)
Zinc Oxide (Internal Mixer Method)5pts.ASTM D 3958-06 (2011)
Stearic Acid (Internal Mixer Method)1pts.ASTM D 3958-06 (2011)
IRB 8 Carbon Black (Internal Mixer Method)40pts.ASTM D 3958-06 (2011)