SUPER SAP® CPM/CPF
- Chemical Family
- Epoxy & Epoxy Derivatives
Super SAP® CPM/CPF is a versatile system designed specifically for the compression molding processes of composite parts. CPM system delivers a high bio-content, excellent fiber wetting qualities, and thixotropic characteristics to limit sag in high-temperature cure applications. A high modulus, combined with excellent elongation properties, enable durable yet lightweight composite parts. CPM is a Super Sap® Formulation.
Properties
- Physical Form
- Liquid
Product families
Applications
- Consumer Goods — Sports & Recreation
- Wall Panels
- Wallcoverings & Decorative Laminates
Product Families
- Thermoset Resins
Other characteristics
- Brand
- SUPER SAP
- End Uses
- Skis, Snowboards
- Polymer Name
- Epoxy Resins & Compounds
- Processing Methods
- Compression Molding
- Markets
- Building & Construction
- Consumer Goods
- Technology
- Composite Materials
- Labeling Claims
- Bio-based
- Application Methods
Recommended for full cure: CPM/CPF—20 minutes at 180°F (82°C). CPM/CPS—40 minutes at 180°F (82°C). Required minimum cure temperature is 150°F (65°C).; For best results, measure the two components by weight within 5% of the recommended mix ratio.; Always mix product for at least two minutes, scraping the container to ensure complete mixing.; Use products in a controlled environment. Avoid high humidity and cold temperatures.; Amine blush, a byproduct of the curing process, appears as a wax-like film on cured epoxy and is more noticeable in cool, moist conditions. It can clog sandpaper and inhibit subsequent bonding. Blush is water-soluble and easily removed with clean water (not solvent) and an abrasive pad.; For good adhesion, epoxy bonding surfaces should be clean, dry, and sanded.; If unfamiliar with the product, create smaller test samples before starting a larger-scale project.
- Composites End Use
- Skis
- Snowboards
- Material Features
- High Durability
- Light Weight
- Certifications and Compliance
- USDA BioPreferred
- USDA Certified Biobased
- Composite Materials Functions
- Resins Binders & Matrix Materials
- Composites Processing Methods
- Compression Molding
Technical data
Table 1 of 1
21 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 435000 | Psi | ASTM D638 |
| Tensile Strength | 8860 | Psi | ASTM D638 |
| Elongation | 6 | % | ASTM D638 |
| Flexural Modulus | 405790 | Psi | ASTM D790 |
| Flexural Strength | 13560 | Psi | ASTM D790 |
| Compression Strength | 12630 | Psi | ASTM D695 |
| Tg Ultimate | 159 | °F | DSC, midpoint |
| Hardness | 70 - 80 | — | Shore D |
| Mix Ratio (by volume) | 2:1 | — | — |
| Mix Ratio (by weight) | 100:42:00 | — | — |
| Viscosity A at 77°F | 1600 | — | — |
| Viscosity B at 77°F | 1700 | — | — |