To catalogue
Toraycon® 1201G-15
- Chemical Family
- Polyesters
Toray Toraycon® 1201G-15 is a Polybutylene Terephthalate (PBT) product filled with 15% glass fiber. It is available in Asia Pacific, Europe, or North America. Typical application Automotive. Primary characteristic includes flame rated.
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Automotive & Transportation — Automotive
- Other Automotive Applications
Electrical & Electronics — Devices & Assemblies
- Other Devices & Assemblies
Electrical & Electronics — Parts & Components
- Housings & Enclosures
- Other Parts & Components
Product Families
Plastics — Engineering & Specialty Polymers
- Polyesters & Copolyesters
Other characteristics
- Brand
- Toraycon
- Polymer Name
- Polybutylene Terephthalate (PBT)
- Fillers Included
- Glass Fiber
- Flexural Modulus
- 5600.0 - 5600.0 MPa
- Processing Methods
- Injection Molding
- Markets
- Automotive & Transportation
- Electrical & Electronics
- Flame Rating
- IEC 60695-11-10 HB
- Technology
- Plastics
- Material Features
- Chemical Resistant
- Dimensional Stability
- Fatigue Resistant
- High Flow
- High Gloss
- Low Water Absorption
- Wear Resistant
- Country Availability
- Brazil
- Canada
- China (Mainland)
- Mexico
- USA
- Plastics and Elastomers End Uses
- Automotive Applications
- Electrical Parts
- Electrical/Electronic Applications
- Housings
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 4
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength | 100 | MPa | ASTM D638 |
| Tensile Modulus | 5900 | MPa | ISO 527 |
| Strain at break | 4 | % | ISO 527 |
| Flexural modulus, 23° | 5600 | MPa | ISO 178 |
| Charpy notched impact strength (+23°) | 5 | kJ/m2 | ISO 179/1eA |
| Charpy impact strength (+23°) | 35 | kJ/m2 | ISO 179/1eU |
| Rockwell Hardness | 90 | Scale M | ISO 2039-2 |
Table 2 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1420 | kg/m3 | ASTM D 792 |
Table 3 of 4
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Coefficient of Linear Thermal Expansion (parallel) | 54 | E-6/K | ISO 11359-1/-2 |
| Temperature of deflection under load (1.80 Mpa) | 200 | °C | ISO 75-1/-2 |
| Temperature of deflection under load (0.45 Mpa) | 220 | °C | ISO 75-1/-2 |
| Thickness tested | 0.4 | mm | — |
| Burning Behavior at thickness | HB | class | IEC 60695-11-10 |
Table 4 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Dissipation factor (1MHz) | 200 | E-4 | IEC 60250 |